Synthesis and characterization of copolymers based on poly(butylene terephthalate) and ethylene oxide-poly(dimethylsiloxane)-ethylene oxide

Vučković, Marija V.; Antić, Vesna; Govedarica, Milutin; Đonlagić, Jasna

(Wiley, 2010)

TY  - JOUR
AU  - Vučković, Marija V.
AU  - Antić, Vesna
AU  - Govedarica, Milutin
AU  - Đonlagić, Jasna
PY  - 2010
UR  - http://TechnoRep.tmf.bg.ac.rs/handle/123456789/5615
AB  - A series of thermoplastic elastomers based on ethylene oxide- poly(dimethylsiloxane)-ethylene oxide (EO-PDMS-EO), as the soft segment, and poly(butylene terephthalate) (PBT), as the hard segment, were synthesized by catalyzed two-step, melt transesterification reaction of dimethyl terephthalate (DMT) with 1, 4-butanediol (BD) and α, ω-dihydroxy-(EO-PDMS-EO). Copolymers with a content of hard PBT segments between 40 and 90 mass % and a constant length of the soft EO-PDMS-EO segments were prepared. The siloxane prepolymer with hydrophilic terminal EO units was used to improve the miscibility between the polar comonomers, DMT and BD, and the nonpolar PDMS. The molecular structure and composition of the copolymers were determined by 1HNMR spectroscopy, whereas the effectiveness of the incorporation of α, ω-dihydroxy-(EO-PDMS-EO) into the copolymer chains was verified by chloroform extraction. The effects of the structure and composition of the copolymers on the melting temperatures and the degree of crystallinity, as well as on the thermal degradation stability and some rheological properties, were studied. It was demonstrated that the degree of crystallinity, the melting and crystallization temperatures of the copolymers increased with increasing mass fraction of the PBT segments. The thermal stability of the copolymers was lower than that of PBT homopolymer, because of the presence of thermoliable ether bonds in the soft segments.
PB  - Wiley
T2  - Journal of Applied Polymer Science
T1  - Synthesis and characterization of copolymers based on poly(butylene terephthalate) and ethylene oxide-poly(dimethylsiloxane)-ethylene oxide
EP  - 3216
IS  - 6
SP  - 3205
VL  - 115
DO  - 10.1002/app.31416
ER  - 
@article{
author = "Vučković, Marija V. and Antić, Vesna and Govedarica, Milutin and Đonlagić, Jasna",
year = "2010",
abstract = "A series of thermoplastic elastomers based on ethylene oxide- poly(dimethylsiloxane)-ethylene oxide (EO-PDMS-EO), as the soft segment, and poly(butylene terephthalate) (PBT), as the hard segment, were synthesized by catalyzed two-step, melt transesterification reaction of dimethyl terephthalate (DMT) with 1, 4-butanediol (BD) and α, ω-dihydroxy-(EO-PDMS-EO). Copolymers with a content of hard PBT segments between 40 and 90 mass % and a constant length of the soft EO-PDMS-EO segments were prepared. The siloxane prepolymer with hydrophilic terminal EO units was used to improve the miscibility between the polar comonomers, DMT and BD, and the nonpolar PDMS. The molecular structure and composition of the copolymers were determined by 1HNMR spectroscopy, whereas the effectiveness of the incorporation of α, ω-dihydroxy-(EO-PDMS-EO) into the copolymer chains was verified by chloroform extraction. The effects of the structure and composition of the copolymers on the melting temperatures and the degree of crystallinity, as well as on the thermal degradation stability and some rheological properties, were studied. It was demonstrated that the degree of crystallinity, the melting and crystallization temperatures of the copolymers increased with increasing mass fraction of the PBT segments. The thermal stability of the copolymers was lower than that of PBT homopolymer, because of the presence of thermoliable ether bonds in the soft segments.",
publisher = "Wiley",
journal = "Journal of Applied Polymer Science",
title = "Synthesis and characterization of copolymers based on poly(butylene terephthalate) and ethylene oxide-poly(dimethylsiloxane)-ethylene oxide",
pages = "3216-3205",
number = "6",
volume = "115",
doi = "10.1002/app.31416"
}
Vučković, M. V., Antić, V., Govedarica, M.,& Đonlagić, J.. (2010). Synthesis and characterization of copolymers based on poly(butylene terephthalate) and ethylene oxide-poly(dimethylsiloxane)-ethylene oxide. in Journal of Applied Polymer Science
Wiley., 115(6), 3205-3216.
https://doi.org/10.1002/app.31416
Vučković MV, Antić V, Govedarica M, Đonlagić J. Synthesis and characterization of copolymers based on poly(butylene terephthalate) and ethylene oxide-poly(dimethylsiloxane)-ethylene oxide. in Journal of Applied Polymer Science. 2010;115(6):3205-3216.
doi:10.1002/app.31416 .
Vučković, Marija V., Antić, Vesna, Govedarica, Milutin, Đonlagić, Jasna, "Synthesis and characterization of copolymers based on poly(butylene terephthalate) and ethylene oxide-poly(dimethylsiloxane)-ethylene oxide" in Journal of Applied Polymer Science, 115, no. 6 (2010):3205-3216,
https://doi.org/10.1002/app.31416 . .
11
14
19

Synthesis and characterization of poly(ester ether siloxane)s

Vučković, Marija V.; Antić, Vesna V.; Dojčinović, Biljana P.; Govedarica, Milutin N.; Đonlagić, Jasna

(John Wiley and Sons Ltd, 2006)

TY  - JOUR
AU  - Vučković, Marija V.
AU  - Antić, Vesna V.
AU  - Dojčinović, Biljana P.
AU  - Govedarica, Milutin N.
AU  - Đonlagić, Jasna
PY  - 2006
UR  - http://TechnoRep.tmf.bg.ac.rs/handle/123456789/5472
AB  - A series of novel thermoplastic elastomers based on ABA-type triblock prepolymers, poly[(propylene oxide)-(dimethylsiloxane)-(propylene oxide)] (PPO-PDMS-PPO), as the soft segments, and poly(butylene terephthalate) (PBT), as the hard segments, was synthesized by catalyzed two-step melt transesterification of dimethyl terephthalate (DMT) with 1,4-butanediol (BD) and α,ω-dihydroxy-(PPO-PDMS-PPO) (M̄ n = 2930 g mol -1 ). Several copolymers with a content of hard PBT segments between 40 and 60 mass% and a constant length of the soft PPO-PDMS-PPO segments were prepared. The siloxane-containing triblock prepolymer with hydrophilic terminal PPO blocks was used to improve the compatibility between the polar comonomers, i.e. DMT and BD, and the non-polar PDMS segments. The structure and composition of the copolymers were examined using 1 H NMR spectroscopy, while the effectiveness of the incorporation of α,ω-dihydroxy-(PPO-PDMS-PPO) prepolymer into the copolyester chains was controlled by chloroform extraction. The effect of the structure and composition of the copolymers on the transition temperatures (T m and T g ) and the thermal and thermo-oxidative degradation stability, as well as on the degree of crystallinity, and some rheological properties, were studied.
PB  - John Wiley and Sons Ltd
T2  - Polymer International
T1  - Synthesis and characterization of poly(ester ether siloxane)s
EP  - 1314
IS  - 11
SP  - 1304
VL  - 55
DO  - 10.1002/pi.2085
ER  - 
@article{
author = "Vučković, Marija V. and Antić, Vesna V. and Dojčinović, Biljana P. and Govedarica, Milutin N. and Đonlagić, Jasna",
year = "2006",
abstract = "A series of novel thermoplastic elastomers based on ABA-type triblock prepolymers, poly[(propylene oxide)-(dimethylsiloxane)-(propylene oxide)] (PPO-PDMS-PPO), as the soft segments, and poly(butylene terephthalate) (PBT), as the hard segments, was synthesized by catalyzed two-step melt transesterification of dimethyl terephthalate (DMT) with 1,4-butanediol (BD) and α,ω-dihydroxy-(PPO-PDMS-PPO) (M̄ n = 2930 g mol -1 ). Several copolymers with a content of hard PBT segments between 40 and 60 mass% and a constant length of the soft PPO-PDMS-PPO segments were prepared. The siloxane-containing triblock prepolymer with hydrophilic terminal PPO blocks was used to improve the compatibility between the polar comonomers, i.e. DMT and BD, and the non-polar PDMS segments. The structure and composition of the copolymers were examined using 1 H NMR spectroscopy, while the effectiveness of the incorporation of α,ω-dihydroxy-(PPO-PDMS-PPO) prepolymer into the copolyester chains was controlled by chloroform extraction. The effect of the structure and composition of the copolymers on the transition temperatures (T m and T g ) and the thermal and thermo-oxidative degradation stability, as well as on the degree of crystallinity, and some rheological properties, were studied.",
publisher = "John Wiley and Sons Ltd",
journal = "Polymer International",
title = "Synthesis and characterization of poly(ester ether siloxane)s",
pages = "1314-1304",
number = "11",
volume = "55",
doi = "10.1002/pi.2085"
}
Vučković, M. V., Antić, V. V., Dojčinović, B. P., Govedarica, M. N.,& Đonlagić, J.. (2006). Synthesis and characterization of poly(ester ether siloxane)s. in Polymer International
John Wiley and Sons Ltd., 55(11), 1304-1314.
https://doi.org/10.1002/pi.2085
Vučković MV, Antić VV, Dojčinović BP, Govedarica MN, Đonlagić J. Synthesis and characterization of poly(ester ether siloxane)s. in Polymer International. 2006;55(11):1304-1314.
doi:10.1002/pi.2085 .
Vučković, Marija V., Antić, Vesna V., Dojčinović, Biljana P., Govedarica, Milutin N., Đonlagić, Jasna, "Synthesis and characterization of poly(ester ether siloxane)s" in Polymer International, 55, no. 11 (2006):1304-1314,
https://doi.org/10.1002/pi.2085 . .
19
13
22

Synthesis of thermoplastic poly(ester-siloxane)s in the melt and in solution

Dojčinović, Biljana; Antić, Vesna; Vučković, Marija V.; Đonlagić, Jasna

(Serbian Chemical Society, 2005)

TY  - JOUR
AU  - Dojčinović, Biljana
AU  - Antić, Vesna
AU  - Vučković, Marija V.
AU  - Đonlagić, Jasna
PY  - 2005
UR  - http://TechnoRep.tmf.bg.ac.rs/handle/123456789/5489
AB  - Two series of thermoplastic elastomers, based on poly(dimethylsiloxane) PDMS, as the soft segment and poly(butylene terephthalate), PBT, as the hard segment, were synthesized by catalyzed transesterification, from dimethyl terephthalate, DMT, silanol-terminated poly(dimethylsiloxane), PDMS-OH Mn=1750g/mol, and 1,4-butanediol, BD. The mole ratio of the starting comonomers was selected to result in a constant hard to soft weight ratio of 55:45. The first series was synthesized in order to determine the optimal mole ratio of BD and DMT for the synthesis of high molecular weight thermoplastic poly(ester-siloxane)s, TPESs. The second series was performed in the presence of the high-boiling solvent, 1,2,4-trichlorbenzene in order to increase the mixing between the extremely non-polar siloxane prepolymer and the polar reactants, DMT and BD, and, therefore, avoid phase separation during synthesis. The structure and composition of the synthesized poly(ester-siloxane)s were verified by 1H-NMR spectroscopy, while the melting temperatures and degree of crystallinity were determined by differential scanning calorimetry (DSC). The effectiveness of the incorporation of the silanol-terminated poly( dimethylsiloxane) into the polyester chains was verified by chloroform extraction. The rheological properties of the poly(ester-siloxane)s were investigated by dynamic mechanical spectroscopy (DMA).
AB  - Dve serije termoplastičnih elastomera na bazi poli(dimetilsiloksana) kao mekog segmenta i poli(butilentereftalata) kao tvrdog segmenta sintetisane su katalizovanom transesterifikacijom polazeći od dimetiltereftalata, DMT silanol-terminarnog poli(dimetil-siloksana), PDMS-OH, Mn=1750g/mol i 1,4-butandiola, BD. Molski odnos početnih komonomera odabran je tako da je rezultovao u konstantnom masenom odnosu tvrdih i mekih segmenata od 55:45. Prva serija je sintetisana sa ciljem da se odredi optimalan molski odnos komonomera BD i DMT za dobijanje termoplastičnih elastomera velikih molarnih masa. U drugoj seriji sinteze su izvođene u prisustvu teško isparljivog rastvarača 1,2,4-trihlorbenzena sa ciljem da se poveća mešljivost izuzetno nepolarnog poli(dimetilsiloksanskog)pretpolimera i polarnih reaktanata, kao što su DMT i BD i samim tim da se izbegne fazna separacija u reakcionoj smeši tokom sinteze. Struktura i sastav sintetisanih poli(estar-siloksana) potvrđeni su 1H-NMR spektroskopijom, dok su temperatura topljenja i stepen kristaliničnosti određeni diferencijalnom skenirajućom kalometrijom (DSC). Efikasnost ugradnje silanol-terminiranog poli(dimetilsiloksana) u poliestarske lance utvrđena je na osnovu ekstrakcije hloroformom. Reološka svojstva poli(estara-siloksana) ispitana su dinamičko-mehaničkom spektroskopijom.
PB  - Serbian Chemical Society
T2  - Journal of the Serbian Chemical Society
T1  - Synthesis of thermoplastic poly(ester-siloxane)s in the melt and in solution
T1  - Sinteza termoplastičnih poli(estar-siloksana) u rastopu i rastvoru
EP  - 1485
IS  - 12
SP  - 1469
VL  - 70
DO  - 10.2298/JSC0512469D
ER  - 
@article{
author = "Dojčinović, Biljana and Antić, Vesna and Vučković, Marija V. and Đonlagić, Jasna",
year = "2005",
abstract = "Two series of thermoplastic elastomers, based on poly(dimethylsiloxane) PDMS, as the soft segment and poly(butylene terephthalate), PBT, as the hard segment, were synthesized by catalyzed transesterification, from dimethyl terephthalate, DMT, silanol-terminated poly(dimethylsiloxane), PDMS-OH Mn=1750g/mol, and 1,4-butanediol, BD. The mole ratio of the starting comonomers was selected to result in a constant hard to soft weight ratio of 55:45. The first series was synthesized in order to determine the optimal mole ratio of BD and DMT for the synthesis of high molecular weight thermoplastic poly(ester-siloxane)s, TPESs. The second series was performed in the presence of the high-boiling solvent, 1,2,4-trichlorbenzene in order to increase the mixing between the extremely non-polar siloxane prepolymer and the polar reactants, DMT and BD, and, therefore, avoid phase separation during synthesis. The structure and composition of the synthesized poly(ester-siloxane)s were verified by 1H-NMR spectroscopy, while the melting temperatures and degree of crystallinity were determined by differential scanning calorimetry (DSC). The effectiveness of the incorporation of the silanol-terminated poly( dimethylsiloxane) into the polyester chains was verified by chloroform extraction. The rheological properties of the poly(ester-siloxane)s were investigated by dynamic mechanical spectroscopy (DMA)., Dve serije termoplastičnih elastomera na bazi poli(dimetilsiloksana) kao mekog segmenta i poli(butilentereftalata) kao tvrdog segmenta sintetisane su katalizovanom transesterifikacijom polazeći od dimetiltereftalata, DMT silanol-terminarnog poli(dimetil-siloksana), PDMS-OH, Mn=1750g/mol i 1,4-butandiola, BD. Molski odnos početnih komonomera odabran je tako da je rezultovao u konstantnom masenom odnosu tvrdih i mekih segmenata od 55:45. Prva serija je sintetisana sa ciljem da se odredi optimalan molski odnos komonomera BD i DMT za dobijanje termoplastičnih elastomera velikih molarnih masa. U drugoj seriji sinteze su izvođene u prisustvu teško isparljivog rastvarača 1,2,4-trihlorbenzena sa ciljem da se poveća mešljivost izuzetno nepolarnog poli(dimetilsiloksanskog)pretpolimera i polarnih reaktanata, kao što su DMT i BD i samim tim da se izbegne fazna separacija u reakcionoj smeši tokom sinteze. Struktura i sastav sintetisanih poli(estar-siloksana) potvrđeni su 1H-NMR spektroskopijom, dok su temperatura topljenja i stepen kristaliničnosti određeni diferencijalnom skenirajućom kalometrijom (DSC). Efikasnost ugradnje silanol-terminiranog poli(dimetilsiloksana) u poliestarske lance utvrđena je na osnovu ekstrakcije hloroformom. Reološka svojstva poli(estara-siloksana) ispitana su dinamičko-mehaničkom spektroskopijom.",
publisher = "Serbian Chemical Society",
journal = "Journal of the Serbian Chemical Society",
title = "Synthesis of thermoplastic poly(ester-siloxane)s in the melt and in solution, Sinteza termoplastičnih poli(estar-siloksana) u rastopu i rastvoru",
pages = "1485-1469",
number = "12",
volume = "70",
doi = "10.2298/JSC0512469D"
}
Dojčinović, B., Antić, V., Vučković, M. V.,& Đonlagić, J.. (2005). Synthesis of thermoplastic poly(ester-siloxane)s in the melt and in solution. in Journal of the Serbian Chemical Society
Serbian Chemical Society., 70(12), 1469-1485.
https://doi.org/10.2298/JSC0512469D
Dojčinović B, Antić V, Vučković MV, Đonlagić J. Synthesis of thermoplastic poly(ester-siloxane)s in the melt and in solution. in Journal of the Serbian Chemical Society. 2005;70(12):1469-1485.
doi:10.2298/JSC0512469D .
Dojčinović, Biljana, Antić, Vesna, Vučković, Marija V., Đonlagić, Jasna, "Synthesis of thermoplastic poly(ester-siloxane)s in the melt and in solution" in Journal of the Serbian Chemical Society, 70, no. 12 (2005):1469-1485,
https://doi.org/10.2298/JSC0512469D . .
8
6
7