Thermal degradation of coordination polymer [Cd(N-Boc-gly)(2)(H2O)(2)](n)
Само за регистроване кориснике
2011
Чланак у часопису (Објављена верзија)
Метаподаци
Приказ свих података о документуАпстракт
Multi-step thermal degradation of coordination polymer [Cd(N-Boc-gly)(2)(H2O)(2)](n) in non-isothermal conditions was studied. The kinetic parameters were determined from the thermal decomposition data using the isoconversion and non-isoconversion techniques. It was shown that the coordination polymer is stable up to 60 C, when the multi-step process of thermal dehydration, followed by steps of degradation, starts. The kinetic triplet for the step of dehydration was established as f(alpha) = 3/2(1 - alpha)(2/3)[1 - (1 - alpha)(1/3)](-1). E-inv = 170.4 +/- 6.4 kJ mol(-1) and Z(inv) =2.6 x 10(23). The established kinetic model, known as "D3 model", was confirmed by application criteria defined by Malek, Perez-Maqueda et al. as well as Master plot method. Dehydration step is followed by two steps of dehydrated coordination polymer degradation. On the base of the dependence of Arrhenius parameters (E-a and Z) on conversion degree (alpha), the mechanisms of degradation were discussed. In th...is way it was shown that second and third steps of degradation of coordination polymer are complex involving more than one elementary step. The second step corresponds to the loss of two C6H5CH2O- fragments in two parallel steps. The third step of degradation, ascribed to the loss of two -C(=O)NHCH2- fragments, is complicated by changing kinetically to diffusion control. (C) 2011 Elsevier B.V. All rights reserved.
Кључне речи:
Coordination polymer / Thermal degradation kinetics / Non isothermal kineticsИзвор:
Thermochimica Acta, 2011, 525, 1-2, 25-30Издавач:
- Elsevier Science Bv, Amsterdam
Финансирање / пројекти:
- Интеракције природних производа, њихових деривата и комплексних једињења са протеинима и нуклеинским киселинама (RS-MESTD-Basic Research (BR or ON)-172055)
- Динамика нелинеарних физичкохемијских и биохемијских система са моделирањем и предвиђањем њихових понашања под неравнотежним условима (RS-MESTD-Basic Research (BR or ON)-172015)
- 0-3D наноструктуре за примену у електроници и обновљивим изворима енергије: синтеза, карактеризација и процесирање (RS-MESTD-Integrated and Interdisciplinary Research (IIR or III)-45007)
DOI: 10.1016/j.tca.2011.07.017
ISSN: 0040-6031
WoS: 000296824400004
Scopus: 2-s2.0-81155159815
Институција/група
Tehnološko-metalurški fakultetTY - JOUR AU - Šumar-Ristović, Maja AU - Anđelković, Katarina K. AU - Poleti, Dejan AU - Minić, Dragica M. PY - 2011 UR - http://TechnoRep.tmf.bg.ac.rs/handle/123456789/5662 AB - Multi-step thermal degradation of coordination polymer [Cd(N-Boc-gly)(2)(H2O)(2)](n) in non-isothermal conditions was studied. The kinetic parameters were determined from the thermal decomposition data using the isoconversion and non-isoconversion techniques. It was shown that the coordination polymer is stable up to 60 C, when the multi-step process of thermal dehydration, followed by steps of degradation, starts. The kinetic triplet for the step of dehydration was established as f(alpha) = 3/2(1 - alpha)(2/3)[1 - (1 - alpha)(1/3)](-1). E-inv = 170.4 +/- 6.4 kJ mol(-1) and Z(inv) =2.6 x 10(23). The established kinetic model, known as "D3 model", was confirmed by application criteria defined by Malek, Perez-Maqueda et al. as well as Master plot method. Dehydration step is followed by two steps of dehydrated coordination polymer degradation. On the base of the dependence of Arrhenius parameters (E-a and Z) on conversion degree (alpha), the mechanisms of degradation were discussed. In this way it was shown that second and third steps of degradation of coordination polymer are complex involving more than one elementary step. The second step corresponds to the loss of two C6H5CH2O- fragments in two parallel steps. The third step of degradation, ascribed to the loss of two -C(=O)NHCH2- fragments, is complicated by changing kinetically to diffusion control. (C) 2011 Elsevier B.V. All rights reserved. PB - Elsevier Science Bv, Amsterdam T2 - Thermochimica Acta T1 - Thermal degradation of coordination polymer [Cd(N-Boc-gly)(2)(H2O)(2)](n) EP - 30 IS - 1-2 SP - 25 VL - 525 DO - 10.1016/j.tca.2011.07.017 ER -
@article{ author = "Šumar-Ristović, Maja and Anđelković, Katarina K. and Poleti, Dejan and Minić, Dragica M.", year = "2011", abstract = "Multi-step thermal degradation of coordination polymer [Cd(N-Boc-gly)(2)(H2O)(2)](n) in non-isothermal conditions was studied. The kinetic parameters were determined from the thermal decomposition data using the isoconversion and non-isoconversion techniques. It was shown that the coordination polymer is stable up to 60 C, when the multi-step process of thermal dehydration, followed by steps of degradation, starts. The kinetic triplet for the step of dehydration was established as f(alpha) = 3/2(1 - alpha)(2/3)[1 - (1 - alpha)(1/3)](-1). E-inv = 170.4 +/- 6.4 kJ mol(-1) and Z(inv) =2.6 x 10(23). The established kinetic model, known as "D3 model", was confirmed by application criteria defined by Malek, Perez-Maqueda et al. as well as Master plot method. Dehydration step is followed by two steps of dehydrated coordination polymer degradation. On the base of the dependence of Arrhenius parameters (E-a and Z) on conversion degree (alpha), the mechanisms of degradation were discussed. In this way it was shown that second and third steps of degradation of coordination polymer are complex involving more than one elementary step. The second step corresponds to the loss of two C6H5CH2O- fragments in two parallel steps. The third step of degradation, ascribed to the loss of two -C(=O)NHCH2- fragments, is complicated by changing kinetically to diffusion control. (C) 2011 Elsevier B.V. All rights reserved.", publisher = "Elsevier Science Bv, Amsterdam", journal = "Thermochimica Acta", title = "Thermal degradation of coordination polymer [Cd(N-Boc-gly)(2)(H2O)(2)](n)", pages = "30-25", number = "1-2", volume = "525", doi = "10.1016/j.tca.2011.07.017" }
Šumar-Ristović, M., Anđelković, K. K., Poleti, D.,& Minić, D. M.. (2011). Thermal degradation of coordination polymer [Cd(N-Boc-gly)(2)(H2O)(2)](n). in Thermochimica Acta Elsevier Science Bv, Amsterdam., 525(1-2), 25-30. https://doi.org/10.1016/j.tca.2011.07.017
Šumar-Ristović M, Anđelković KK, Poleti D, Minić DM. Thermal degradation of coordination polymer [Cd(N-Boc-gly)(2)(H2O)(2)](n). in Thermochimica Acta. 2011;525(1-2):25-30. doi:10.1016/j.tca.2011.07.017 .
Šumar-Ristović, Maja, Anđelković, Katarina K., Poleti, Dejan, Minić, Dragica M., "Thermal degradation of coordination polymer [Cd(N-Boc-gly)(2)(H2O)(2)](n)" in Thermochimica Acta, 525, no. 1-2 (2011):25-30, https://doi.org/10.1016/j.tca.2011.07.017 . .