dc.creatorMilović, Ljubica
dc.creatorSedmak, Aleksandar
dc.creatorBlačić, Ivo
dc.creatorVuherer, Tomaž
dc.creatorPetrovski, Blagoj
dc.date.accessioned2023-05-29T08:59:26Z
dc.date.available2023-05-29T08:59:26Z
dc.date.issued2022
dc.identifier.isbn978-171387030-2
dc.identifier.issn2452-3216
dc.identifier.urihttp://TechnoRep.tmf.bg.ac.rs/handle/123456789/6428
dc.description.abstractIn order to assess the integrity of welded pressure vessel containing a crack, the behavior of three-point bending specimens made of HSLA steel welded joint are tested at -40 °C, and their fracture behaviour analyzed, as a conservative measure of crack resistance. Specimens were made of low-alloyed steel NIONIKRAL 70, welded by SAW process. Surface notches were machined by the electro-erosion method in the parent metal (PM), heat affected zone (HAZ) and weld metal (WM). The highest resistance to cracking was in PM, and the lowest one in WM, due to so-called pop-in behaviour.sr
dc.language.isoensr
dc.publisherElsevier B.V.sr
dc.relationinfo:eu-repo/grantAgreement/MESTD/inst-2020/200105/RS//sr
dc.relationinfo:eu-repo/grantAgreement/MESTD/inst-2020/200135/RS//sr
dc.rightsopenAccesssr
dc.rights.urihttps://creativecommons.org/licenses/by-nc-nd/4.0/
dc.source23rd European Conference on Fracture, ECF 2022, Procedia Structural Integritysr
dc.subjectfracturesr
dc.subjectHSLAsr
dc.subjectSEM micrographssr
dc.subjectweldingsr
dc.titleExperimental Analysis of HSLA Steel Welded Joint Fracture Behavioursr
dc.typeconferenceObjectsr
dc.rights.licenseBY-NC-NDsr
dc.citation.epage1502
dc.citation.spage1497
dc.citation.volume42
dc.identifier.doi10.1016/j.prostr.2022.12.190
dc.identifier.fulltexthttp://TechnoRep.tmf.bg.ac.rs/bitstream/id/17205/1-s2.0-S2452321622007478-main.pdf
dc.identifier.scopus2-s2.0-85158974865
dc.type.versionpublishedVersionsr