Influence of the alkali treatment on the sorption and dielectric properties of woven jute fabric
(Springer, 2019)
Woven jute fabric was treated with sodium hydroxide solution of different concentrations at room temperature, for different periods of time. After that, jute fabrics with gradually decreased content of hemicelluloses were ...
Surface cleaning of raw cotton fibers with atmospheric pressure air plasma
(Springer, Dordrecht, 2018)
In this work, a possibility to use atmospheric pressure plasma treatment to clean cotton fibers surface was investigated. Dielectric barrier discharge (DBD) operating in air was used as plasma source. After plasma treatment, ...
In situ photoreduction of Ag+-ions on the surface of titania nanotubes deposited on cotton and cotton/PET fabrics
(Springer, Dordrecht, 2017)
This study discusses the possibility of in situ photoreduction of Ag+-ions on the surface of titania nanotubes (TNTs) deposited on the cotton and cotton/PET fabrics in the presence of amino acid alanine and methyl alcohol. ...
Preparation of cellulosic fibers with biological activity by immobilization of trypsin on periodate oxidized viscose fibers
(Springer, Dordrecht, 2014)
In this study, a biologically active fibrous material was designed by immobilizing trypsin on viscose fibers. The viscose yarn was first oxidized with sodium periodate to produce aldehyde groups and then employed as a ...
Electrokinetic and sorption properties of hydrogen peroxide treated flax fibers (Linum usitatissimum L.)
(Cellulose, 2021)
Hydrogen peroxide represents an ecologically and economically acceptable agent for bleaching of flax fibers. The influence of hydrogen peroxide treatment under different conditions, i.e. hydrogen peroxide concentrations ...
Nitrogen plasma surface treatment for improving polar ink adhesion on micro/nanofibrillated cellulose films
(Springer, Dordrecht, 2019)
We find that nitrogen plasma treatment of micro/nanofibrillated cellulose films increases wettability of the surface by both liquid polar water and nonpolar hexadecane. The increased wetting effect is more pronounced in ...
Halochromic cellulose textile obtained via dyeing with biocolorant isolated from Streptomyces sp. strain NP4
(Cellulose, 2021)
Halochromic (pH-responsive) material was obtained by dyeing functionalized viscose fabric with a crude extract from Streptomyces sp. strain NP4. The functionalization of the fabric before dyeing was performed to make ...
Study of interaction between nitrogen DBD plasma-treated viscose fibers and divalent ions Ca2+ and Cu2+
(Springer, Dordrecht, 2014)
Viscose fibers were treated with atmospheric pressure dielectric barrier discharge (DBD) plasma obtained in nitrogen in order to activate the fiber surface prior to sorption of the divalent ions Ca2+ and Cu2+. Methylene ...
TEMPO-oxidized cotton as a substrate for trypsin immobilization: impact of functional groups on proteolytic activity and stability
(Springer, Dordrecht, 2017)
Cotton fibers containing different amounts of aldehyde and carboxyl groups were prepared by varying TEMPO oxidation conditions and then employed as carriers for trypsin immobilization. Depending on the functional group ...
Influence of hemicelluloses and lignin content on structure and sorption properties of flax fibers (Linum usitatissimum L.)
(Springer, Dordrecht, 2018)
In this work, alkali and oxidative treatments were employed to obtain flax fibers with different content of hemicelluloses and lignin, in order to study the influence of chemical composition on structure and sorption ...