Pretraživanje
Prikaz rezultata 1-10 od 24
Non-isothermal crystallization of k2o center dot tio2 center dot 3geo(2) glass
(Springer, Dordrecht, 2009)
The crystallization of K2O center dot TiO2 center dot 3GeO(2) glass under non-isothermal condition was studied. In powdered glass with particle sizes less than 0.15 mm, surface crystallization was dominant and an activation ...
The kinetics of the thermal degradation of isomeric dipropyl and dibutyl esters of poly(itaconic acid)
(Pergamon-Elsevier Science Ltd, Oxford, 2000)
Non-oxidative and oxidative thermogravimetry was performed on poly(di-n-propyl-) (PDnPI), poly(di-iso-propyl-) (PDiPI), poly(di-n-butyl-) (PDnBI), poly(di-iso-butyl-) (PDiBI) and poly(di-sec-butyl itaconate) (PDsBI). The ...
The thermal degradation kinetics of isomeric poly(dipropyl, itaconates)
(Springer, Dordrecht, 1997)
Non-isothermal thermogravimetry was performed in a dynamic nitrogen atmosphere, on a series of poly(di-n-propyl itaconates) (PDnPI) and poly(di-iso-propyl itaconates) (PDiPI) which had been prepared in the presence of ...
The thermal degradation kinetics of poly(chlorethylmethacrylates)
(John Wiley & Sons Ltd, W Sussex, 1992)
The thermal degradation kinetics of poly(2-mono-, 2,2-di- and 2,2,2-trichlorethyl methacrylate) and of the non-chlorinated poly(ethyl methacrylate) were studied by TG in the absence and presence of oxygen. The overall ...
Factors influencing the removal of divalent cations by hydroxyapatite
(Elsevier, Amsterdam, 2008)
The effect of pH, contact time, initial metal concentration and presence of common competing cations, on hydroxyapatite (HAP) sorption properties towards Ph2+, Cd2+, Zn2+, and Sr2+ ions was studied and compared using a ...
The thermal degradation kinetics of dextran and pullulan
(John Wiley & Sons Ltd, W Sussex, 1993)
The effect of molar mass and, in the case of dextran, of the degree of branching on the thermal degradation kinetics of dextran and pullulan was studied in the presence and absence of oxygen. Although the initial mass loss ...
The non-oxidative thermal degradation of poly (Di-2-chloroethyl itaconate)
(John Wiley & Sons Ltd, W Sussex, 1993)
The non-oxidative thermal degradation of poly (di-2-chloroethyl itaconate) (PD2CEI) was studied by TG and by analysing the thermal products. The major processes occurring during thermal analysis are crosslinking, ...
Kinetic properties of the Ti-Ni intermetallic phases and alloys for hydrogen evolution
(Elsevier Science Sa, Lausanne, 1997)
The kinetics and mechanism of hydrogen evolution at Ti-Ni alloy electrodes prepared by are-melting and mechanical alloying methods has been studied by means of AC impedance spectrum measurements. The electrode, prepared ...
The thermal degradation of poly(diethyl fumarate)
(Elsevier Sci Ltd, Oxford, 2006)
The kinetics and mechanism of the thermal degradation of poly(diethyl fumarate) (PDEF) were studied by thermogravimetry, as well as by analysis of the thermolysis volatiles and polymer residue. The characteristic mass loss ...
Applications of non-linear frequency response for investigation of adsorption systems
(Soc Chemists Technologists Madeconia, Skopje, 2009)
Two main directions of application of nonlinear frequency response and the concept of higher order frequency response functions (FRFs) in investigation of adsorption systems are presented, one for development of novel ...