Properties of dispersion-hardened copper made by internal oxidation of prealloyed copper powder containing 2.5wt. % Al
(Trans Tech Publications Ltd, Durnten-Zurich, 2005)
Prealloyed copper powder containing 2.5wt. %Al was processed in a planetary ball mill to evaluate matrix hardening due to formation of Al2O3 particles in situ by internal oxidation. After milling, the powders were heat ...