Application of instrumental methods in the investigation of properties and microstructure of construction concretes / Primena instrumentalnih metoda za ispitivanje svojstava i mikrostrukture konstukcionih betona
(Savez inženjera metalurgije Srbije, Beograd, 2008)
Methods for the investigation of microstructure of construction concretes are presented in this paper. Concrete is a composite material, thus its microstructure consists of bonding agent (cement) and aggregate with predefined ...
Uticaj strukture na sposobnost oblikovanja Al-Mg6,8 legure / Influence of microstructure on the formability of Al-Mg6.8 alloy
(Association of Chemical Engineers of Serbia, 2008)
U ovom radu korišćena je aluminijum-magnezijum legura sa 6,8% magnezijuma (Al-Mg6,8), koja pripada grupi Al-Mg legura visoke čvrstoće. Ispitivan je uticaj mikrostrukture, koja se postiže primenom različitih uslova ...