Determination of Degradation Level during Cavitation Erosion of Zircon Based Ceramic
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2017)
Mechanical shock of zircon based ceramic induced by cavitation erosion testing was investigated in this study. Several parameters were followed in order to determine level of material degradation during the cavitation ...
Thermal Shock Properties of Glass-ceramics Synthesized From a Glass Frit
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2017)
In this study, the behavior of glass-ceramics synthesized from a glass frit of FFW (Final Flotation Waste) originated from the RTB Bor Company was investigated. Thermal shock resistance was monitored in order to assess the ...
Structural, Chemical and Magnetic Properties of Nickel Vertical Posts Obtained by Glancing Angle Deposition Technique
(Science of Sintering, 2017)
In this work, Glancing Angle Deposition technique was used for obtaining nanostructured nickel thin film with vertical posts on glass substrate which was positioned 75 degrees with respect to the substrate normal and rotated ...
Formation of Porous Wollastonite-based Ceramics after Sintering With Yeast as the Pore-forming Agent
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2017)
In this paper, synthesis of porous wollastonite-based ceramics was reported. Ceramic precursor, methylhydrocyclosiloxane, together with micro-sized CaCO3, was used as starting material. After 20 min of ultrasound treatment, ...
Sol-gel Synthesis of Anatase Nanopowders for Efficient Photocatalytic Degradation of Herbicide Clomazone in Aqueous Media
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2017)
TiO2 nanopowders were produced by sol-gel technique using TiCl4 as a starting material. For the preparation of crystalline anatase with developed surface area, this aqueous solution has been mixed with 0.05 M or 0.07 M ...