Termooksidativna degradacija poli(2-hloretil metakrilata) u prisustvu antioksidanata

dc.creatorŽagar, Maja J.
dc.creatorKatsikas, Lynne
dc.creatorPopović, Ivanka
dc.date.accessioned2021-03-10T09:52:41Z
dc.date.available2021-03-10T09:52:41Z
dc.date.issued2000
dc.identifier.issn0367-598X
dc.identifier.urihttp://TechnoRep.tmf.bg.ac.rs/handle/123456789/310
dc.description.abstractThe oxidative thermal degradation of poly(2-chloroethyl methacrylate) (PCEMA) was studied in the presence of the following commercial antioxidants: CHIMASSORB 119 (CH 119) and CHIMASSORB 944 (CH 944), both based on amines, and a mixture of IRGANOX 1010, a phenol derivative, and IRGAPHOS 168, a phosphite (mass ratio 1:1), by the thermogravimetric (TG) method. On the basis of the obtained results, the characteristic temperatures of 10% mass loss, Tio%, the shape of the differential TG (DTG) curves and mean values of the thermal degradation activation energy, Ea, it was concluded that the commercial photostabilisers CH 119 and CH 944 could not successfully stabilize the thermal degradation of PCEMA, while in the case of the presence of the antioxidant mixture IRGANOX 1010 and IRGAPHOS 168 (1:1) slight stabilizing effects were observed.en
dc.description.abstractU radu je ispitana oksidativna termijska degradacija poli(2-hloretil metakrilata) (PCEMA) u prisustvu komercijalnih antioksidanata amino tipa CHIMASSORB 119 (CH 119) i CHIMASSORB 944 (CH 944) i smeše antioksidanata, IRGANOX 1010, fenolnog derivata, i IRGAPHOS 168, fosfita (maseni udeli 1:1). Ispitivanja su izvedena termogravimetrijskom (TG) metodom, a na osnovu karakterističnih temperatura 10% gubitka mase, oblika diferencijalnih TG (DTG) krivih i srednjih vrednosti energije aktivacije termijske degradacije, ispitivan je uticaj pojedinih antioksidanata.sr
dc.publisherAssociation of Chemical Engineers of Serbia
dc.rightsopenAccess
dc.rights.urihttps://creativecommons.org/licenses/by-nc-nd/4.0/
dc.sourceHemijska industrija
dc.subjectthermo-oxidative degradationen
dc.subjectpolymethacrylatesen
dc.subjectantioxidantsen
dc.subjectthermogravimetryen
dc.subjecttermooksidativna degradacijasr
dc.subjectpolimetakrilatisr
dc.subjectantioksidantisr
dc.subjecttermogravimetrijasr
dc.titleThe thermo-oxidative degradation of poly(2-chloroethyl methacrylate) in the presence of antioxidantsen
dc.titleTermooksidativna degradacija poli(2-hloretil metakrilata) u prisustvu antioksidanatasr
dc.typearticle
dc.rights.licenseBY-NC-ND
dc.citation.epage341
dc.citation.issue7-8
dc.citation.other54(7-8): 337-341
dc.citation.spage337
dc.citation.volume54
dc.identifier.rcubhttps://hdl.handle.net/21.15107/rcub_technorep_310
dc.type.versionpublishedVersion


Документи

ДатотекеВеличинаФорматПреглед

Уз овај запис нема датотека.

Овај документ се појављује у следећим колекцијама

Приказ основних података о документу