TechnoRep - Faculty of Technology and Metallurgy Repository
University of Belgrade - Faculty of Technology and Metallurgy
    • English
    • Српски
    • Српски (Serbia)
  • English 
    • English
    • Serbian (Cyrillic)
    • Serbian (Latin)
  • Login
View Item 
  •   TechnoRep
  • Tehnološko-metalurški fakultet
  • Radovi istraživača / Researchers’ publications (TMF)
  • View Item
  •   TechnoRep
  • Tehnološko-metalurški fakultet
  • Radovi istraživača / Researchers’ publications (TMF)
  • View Item
JavaScript is disabled for your browser. Some features of this site may not work without it.

Initial microstructure effect on the mechanical properties of Ti-6Al-4V ELI alloy processed by high-pressure torsion

Authorized Users Only
2018
Authors
Cvijović-Alagić, Ivana
Cvijović, Zorica
Maletaškić, Jelena
Rakin, Marko
Article (Published version)
Metadata
Show full item record
Abstract
effect of initial microstructure on the mechanical properties and fracture mode of the Ti-6Al-4V ELI alloy subjected to the high-pressure torsion (HPT) processing at room temperature and 500 degrees C was investigated. In this purpose, the four different microstructures (fully lamellar, martensitic, equiaxed and globular microstructures) were developed by the proper heat treatments. The results showed that the application of the HPT processing provided substantial microstructural refinement, independent on the alloy initial microstructure. As a consequence, the alloy hardness, tensile strength and ductility significantly increased. At the same time, the elastic modulus of the HPT-processed alloy is almost 2 times lower as compared to that of the alloy in the initial heat treated state. The obtained improvements strongly depend on the alloy initial microstructure and HPT processing temperature. It was found that the initial martensitic microstructure is beneficial to improve the hardnes...s, tensile and fracture properties. The HPT processing at 500 degrees C enhanced them more effectively. After the warm HPT processing, alloy with the initial martensitic microstructure exhibited exceptional hardness (455 MPa), high ultimate tensile strength (1546 MPa), high elongation to failure (18.8%) and low elastic modulus (78.6 GPa). Although the alloy with initial fully lamellar microstructure displayed the lowest elastic modulus (68 GPa), the ultrafine and homogeneous (alpha + beta) two-phase microstructure produced by the HPT processing of the alloy with initial martensitic microstructure offered the best combination of the strength-ductility balance and strength-to-elastic modulus ratio (19.8 x 10(-3)). The complex fracture process, involving transgranular quasi-cleavage and ductile dimple fracture mode, corresponded to the changes in ductility.

Keywords:
Ti-based alloy / High-pressure torsion / Microstructure / Mechanical properties / Fracture
Source:
Materials Science and Engineering A-Structural Materials Properties Microstructure and Processing, 2018, 736, 175-192
Publisher:
  • Elsevier Science Sa, Lausanne
Funding / projects:
  • Micromechanical criteria of damage and fracture (RS-174004)
  • Erich Schmid Institute of Materials Science, Austrian Academy of Sciences, Leoben, Austria
  • Laboratory for Advanced Nuclear Energy, Institute of Innovative Research, Tokyo Institute of Technology, Tokyo, Japan

DOI: 10.1016/j.msea.2018.08.094

ISSN: 0921-5093

WoS: 000447573400019

Scopus: 2-s2.0-85052870387
[ Google Scholar ]
4
URI
http://TechnoRep.tmf.bg.ac.rs/handle/123456789/3929
Collections
  • Radovi istraživača / Researchers’ publications (TMF)
Institution/Community
Tehnološko-metalurški fakultet
TY  - JOUR
AU  - Cvijović-Alagić, Ivana
AU  - Cvijović, Zorica
AU  - Maletaškić, Jelena
AU  - Rakin, Marko
PY  - 2018
UR  - http://TechnoRep.tmf.bg.ac.rs/handle/123456789/3929
AB  - effect of initial microstructure on the mechanical properties and fracture mode of the Ti-6Al-4V ELI alloy subjected to the high-pressure torsion (HPT) processing at room temperature and 500 degrees C was investigated. In this purpose, the four different microstructures (fully lamellar, martensitic, equiaxed and globular microstructures) were developed by the proper heat treatments. The results showed that the application of the HPT processing provided substantial microstructural refinement, independent on the alloy initial microstructure. As a consequence, the alloy hardness, tensile strength and ductility significantly increased. At the same time, the elastic modulus of the HPT-processed alloy is almost 2 times lower as compared to that of the alloy in the initial heat treated state. The obtained improvements strongly depend on the alloy initial microstructure and HPT processing temperature. It was found that the initial martensitic microstructure is beneficial to improve the hardness, tensile and fracture properties. The HPT processing at 500 degrees C enhanced them more effectively. After the warm HPT processing, alloy with the initial martensitic microstructure exhibited exceptional hardness (455 MPa), high ultimate tensile strength (1546 MPa), high elongation to failure (18.8%) and low elastic modulus (78.6 GPa). Although the alloy with initial fully lamellar microstructure displayed the lowest elastic modulus (68 GPa), the ultrafine and homogeneous (alpha + beta) two-phase microstructure produced by the HPT processing of the alloy with initial martensitic microstructure offered the best combination of the strength-ductility balance and strength-to-elastic modulus ratio (19.8 x 10(-3)). The complex fracture process, involving transgranular quasi-cleavage and ductile dimple fracture mode, corresponded to the changes in ductility.
PB  - Elsevier Science Sa, Lausanne
T2  - Materials Science and Engineering A-Structural Materials Properties Microstructure and Processing
T1  - Initial microstructure effect on the mechanical properties of Ti-6Al-4V ELI alloy processed by high-pressure torsion
EP  - 192
SP  - 175
VL  - 736
DO  - 10.1016/j.msea.2018.08.094
UR  - conv_5686
ER  - 
@article{
author = "Cvijović-Alagić, Ivana and Cvijović, Zorica and Maletaškić, Jelena and Rakin, Marko",
year = "2018",
abstract = "effect of initial microstructure on the mechanical properties and fracture mode of the Ti-6Al-4V ELI alloy subjected to the high-pressure torsion (HPT) processing at room temperature and 500 degrees C was investigated. In this purpose, the four different microstructures (fully lamellar, martensitic, equiaxed and globular microstructures) were developed by the proper heat treatments. The results showed that the application of the HPT processing provided substantial microstructural refinement, independent on the alloy initial microstructure. As a consequence, the alloy hardness, tensile strength and ductility significantly increased. At the same time, the elastic modulus of the HPT-processed alloy is almost 2 times lower as compared to that of the alloy in the initial heat treated state. The obtained improvements strongly depend on the alloy initial microstructure and HPT processing temperature. It was found that the initial martensitic microstructure is beneficial to improve the hardness, tensile and fracture properties. The HPT processing at 500 degrees C enhanced them more effectively. After the warm HPT processing, alloy with the initial martensitic microstructure exhibited exceptional hardness (455 MPa), high ultimate tensile strength (1546 MPa), high elongation to failure (18.8%) and low elastic modulus (78.6 GPa). Although the alloy with initial fully lamellar microstructure displayed the lowest elastic modulus (68 GPa), the ultrafine and homogeneous (alpha + beta) two-phase microstructure produced by the HPT processing of the alloy with initial martensitic microstructure offered the best combination of the strength-ductility balance and strength-to-elastic modulus ratio (19.8 x 10(-3)). The complex fracture process, involving transgranular quasi-cleavage and ductile dimple fracture mode, corresponded to the changes in ductility.",
publisher = "Elsevier Science Sa, Lausanne",
journal = "Materials Science and Engineering A-Structural Materials Properties Microstructure and Processing",
title = "Initial microstructure effect on the mechanical properties of Ti-6Al-4V ELI alloy processed by high-pressure torsion",
pages = "192-175",
volume = "736",
doi = "10.1016/j.msea.2018.08.094",
url = "conv_5686"
}
Cvijović-Alagić, I., Cvijović, Z., Maletaškić, J.,& Rakin, M.. (2018). Initial microstructure effect on the mechanical properties of Ti-6Al-4V ELI alloy processed by high-pressure torsion. in Materials Science and Engineering A-Structural Materials Properties Microstructure and Processing
Elsevier Science Sa, Lausanne., 736, 175-192.
https://doi.org/10.1016/j.msea.2018.08.094
conv_5686
Cvijović-Alagić I, Cvijović Z, Maletaškić J, Rakin M. Initial microstructure effect on the mechanical properties of Ti-6Al-4V ELI alloy processed by high-pressure torsion. in Materials Science and Engineering A-Structural Materials Properties Microstructure and Processing. 2018;736:175-192.
doi:10.1016/j.msea.2018.08.094
conv_5686 .
Cvijović-Alagić, Ivana, Cvijović, Zorica, Maletaškić, Jelena, Rakin, Marko, "Initial microstructure effect on the mechanical properties of Ti-6Al-4V ELI alloy processed by high-pressure torsion" in Materials Science and Engineering A-Structural Materials Properties Microstructure and Processing, 736 (2018):175-192,
https://doi.org/10.1016/j.msea.2018.08.094 .,
conv_5686 .

DSpace software copyright © 2002-2015  DuraSpace
About TechnoRep | Send Feedback

OpenAIRERCUB
 

 

All of DSpaceInstitutions/communitiesAuthorsTitlesSubjectsThis institutionAuthorsTitlesSubjects

Statistics

View Usage Statistics

DSpace software copyright © 2002-2015  DuraSpace
About TechnoRep | Send Feedback

OpenAIRERCUB