Biomimetic characterization reveals enhancement of hydroxyapatite formation by fluid flow in gellan gum and bioactive glass composite scaffolds (vol 76, pg 464, 2019)
dc.creator | Zvicer, Jovana | |
dc.creator | Medić, Ana | |
dc.creator | Veljović, Đorđe | |
dc.creator | Jevtić, Sanja | |
dc.creator | Novak, Sasa | |
dc.creator | Obradović, Bojana | |
dc.date.accessioned | 2021-03-10T13:54:05Z | |
dc.date.available | 2021-03-10T13:54:05Z | |
dc.date.issued | 2019 | |
dc.identifier.issn | 0142-9418 | |
dc.identifier.uri | http://TechnoRep.tmf.bg.ac.rs/handle/123456789/4051 | |
dc.description.abstract | The authors regret that Figures 4 and 5 in the above manuscript were exchanged. The authors would like to apologise for any inconvenience caused. | |
dc.publisher | Elsevier Sci Ltd, Oxford | |
dc.rights | restrictedAccess | |
dc.source | Polymer Testing | |
dc.title | Biomimetic characterization reveals enhancement of hydroxyapatite formation by fluid flow in gellan gum and bioactive glass composite scaffolds (vol 76, pg 464, 2019) | en |
dc.type | contributionToPeriodical | |
dc.rights.license | ARR | |
dc.citation.other | 77: - | |
dc.citation.rank | M21 | |
dc.citation.spage | 105908 | |
dc.citation.volume | 77 | |
dc.identifier.doi | 10.1016/j.polymertesting.2019.105908 | |
dc.identifier.scopus | 2-s2.0-85065792149 | |
dc.identifier.wos | 000487002700043 | |
dc.type.version | publishedVersion |