Characterization of vacuum plasma spray VPS - W coating deposited on stainless steel substrates / Karakterizacija vakuum plazma sprej VPS - W prevlake deponovane na čeličnim podloga
(Inženjersko društvo za koroziju, 2021)
In this paper, studied was the melting of W powder particles in plasma, their behavior at oxidation as well as the mechanism of hardening on the surface of the substrate. Tungsten coating layers were deposited with vacuum ...
Characterisation of biocompatible layers of ZrO28%Y2O used in combination with other ceramics to modify the surface of implants / Karakterizacija biokompatibilnih slojeva ZrO28%Y2O3 koji se koriste u kombinaciji sa drugom keramikom za modifikaciju površine implantata
(Inženjersko društvo za koroziju, 2021)
The aim of this study was to deposit multi-functional ZrO28%Y2O3 coating layers using the plasma spray technology and then to characterise such layers. In combination with other biomedical ceramics, this coating is intended ...