Претраживање
Приказ резултата 1-5 од 5
INTEGRITY AND RISK ASSESSMENT OF RECONSTRUCTED STEAM LINE / PROCENA INTEGRITETA I RIZIKA REKONSTRUISANOG PAROVODA
(Society for Structural Integrity and Life (DIVK), 2023)
The integrity assessment of high pressure steam pipeline
primarily requires stress state determination, including not
only effects of working pressure and temperature, but also
all acting loads. Toward this aim, the ...
Characterization of vacuum plasma spray VPS - W coating deposited on stainless steel substrates / Karakterizacija vakuum plazma sprej VPS - W prevlake deponovane na čeličnim podloga
(Inženjersko društvo za koroziju, 2021)
In this paper, studied was the melting of W powder particles in plasma, their behavior at oxidation as well as the mechanism of hardening on the surface of the substrate. Tungsten coating layers were deposited with vacuum ...
Characterisation of biocompatible layers of ZrO28%Y2O used in combination with other ceramics to modify the surface of implants / Karakterizacija biokompatibilnih slojeva ZrO28%Y2O3 koji se koriste u kombinaciji sa drugom keramikom za modifikaciju površine implantata
(Inženjersko društvo za koroziju, 2021)
The aim of this study was to deposit multi-functional ZrO28%Y2O3 coating layers using the plasma spray technology and then to characterise such layers. In combination with other biomedical ceramics, this coating is intended ...
Characterization of NiAl layers deposited by atmospheric plasma spray (APS) / Karakterizacija NiAl slojeva deponovanih atmosferskim plazma sprejom (APS)
(Engineering Society for Corrosion, Belgrade, Serbia, 2020)
In this paper analyzed were the mechanical properties and microstructure of the Ni30Al coating layers deposited using atmospheric plasma spray (APS). For deposition of the coating applied was a composite Ni30wt.% Al powder, ...
The mechanical and microstructural properties of VPS-Ti porous coating deposited on titanium alloy substrates for osseointegration / Mehanička i mikrostrukturna svojstva VPS-Ti porozne prevlake deponovane na podlogama od legure titana za osteointegraciju
(Engineering Society for Corrosion, Belgrade, Serbia, 2020)
The topography of the surface of the deposited VPS-Ti coatings on substrate surfaces of implants relating to the roughness and porous structure plays a decisive role in the process of on growth of the implants to the bones ...