INTEGRITY AND RISK ASSESSMENT OF RECONSTRUCTED STEAM LINE / PROCENA INTEGRITETA I RIZIKA REKONSTRUISANOG PAROVODA
(Society for Structural Integrity and Life (DIVK), 2023)
The integrity assessment of high pressure steam pipeline
primarily requires stress state determination, including not
only effects of working pressure and temperature, but also
all acting loads. Toward this aim, the ...
Characterization of NiAl layers deposited by atmospheric plasma spray (APS) / Karakterizacija NiAl slojeva deponovanih atmosferskim plazma sprejom (APS)
(Engineering Society for Corrosion, Belgrade, Serbia, 2020)
In this paper analyzed were the mechanical properties and microstructure of the Ni30Al coating layers deposited using atmospheric plasma spray (APS). For deposition of the coating applied was a composite Ni30wt.% Al powder, ...
The mechanical and microstructural properties of VPS-Ti porous coating deposited on titanium alloy substrates for osseointegration / Mehanička i mikrostrukturna svojstva VPS-Ti porozne prevlake deponovane na podlogama od legure titana za osteointegraciju
(Engineering Society for Corrosion, Belgrade, Serbia, 2020)
The topography of the surface of the deposited VPS-Ti coatings on substrate surfaces of implants relating to the roughness and porous structure plays a decisive role in the process of on growth of the implants to the bones ...