Characterisation of biocompatible layers of ZrO28%Y2O used in combination with other ceramics to modify the surface of implants / Karakterizacija biokompatibilnih slojeva ZrO28%Y2O3 koji se koriste u kombinaciji sa drugom keramikom za modifikaciju površine implantata
(Inženjersko društvo za koroziju, 2021)
The aim of this study was to deposit multi-functional ZrO28%Y2O3 coating layers using the plasma spray technology and then to characterise such layers. In combination with other biomedical ceramics, this coating is intended ...
The mechanical and microstructural properties of VPS-Ti porous coating deposited on titanium alloy substrates for osseointegration / Mehanička i mikrostrukturna svojstva VPS-Ti porozne prevlake deponovane na podlogama od legure titana za osteointegraciju
(Engineering Society for Corrosion, Belgrade, Serbia, 2020)
The topography of the surface of the deposited VPS-Ti coatings on substrate surfaces of implants relating to the roughness and porous structure plays a decisive role in the process of on growth of the implants to the bones ...
Characterization of NiAl layers deposited by atmospheric plasma spray (APS) / Karakterizacija NiAl slojeva deponovanih atmosferskim plazma sprejom (APS)
(Engineering Society for Corrosion, Belgrade, Serbia, 2020)
In this paper analyzed were the mechanical properties and microstructure of the Ni30Al coating layers deposited using atmospheric plasma spray (APS). For deposition of the coating applied was a composite Ni30wt.% Al powder, ...