dc.description.abstractFormability of Al-Mg4.5-Cu0.5 alloy sheets was tested after annealing at different temperatures (220-520 degrees C) and water quenching. The formability (normalized limiting dome heights, LDH/R) showed only a small variation for all the samples with recrystallized structure, i.e. the LDH/R-e(2) curves were within similar to 13% in the range of plane strain deformation. The samples annealed at 280 degrees C experienced a formability level at the upper limit of the band containing all the LDHIR values. The formability rating seems to be the result of the complex interaction of the strain hardening ability and strain rate sensitivity (SRS) due to different structural features developed during different annealing conditions.en
dc.publisherElsevier Science Sa, Lausanne
dc.rightsrestrictedAccess
dc.sourceJournal of Materials Processing Technology
dc.subjectAl-Mg-Cu sheeten
dc.subjectprecipitationen
dc.subjectstrain hardeningen
dc.subjectstrain rate sensitivityen
dc.subjectformabilityen
dc.titleEffect of annealing temperature on the formability of Al-Mg4.5-Cu0.5 alloy sheetsen
dc.typearticle
dc.rights.licenseARR
dc.citation.epage389
dc.citation.issue1-3
dc.citation.other177(1-3): 386-389
dc.citation.rankM22
dc.citation.spage386
dc.citation.volume177
dc.identifier.doi10.1016/j.jmatprotec.2006.04.036
dc.identifier.scopus2-s2.0-33745961343
dc.identifier.wos000239611900086
dc.type.versionpublishedVersion


Документи

Thumbnail

Овај документ се појављује у следећим колекцијама

Приказ основних података о документу