Durability of sulfur concrete with different fillers, as well as Portland cement concrete, was tested in the solutions of HCl, H(2)SO(4), and NaCl. Regarding mass changes, in the solutions of HCl and H(2)SO(4) sulfur concrete with talc and fly ash exhibited higher durability, while in NaCl samples with alumina and microsilica were better. The type of filler did not affect durability regarding compressive strength. Strength loss was higher in the solution of HCl comparing to H(2)SO(4), while negligible in NaCl which is in accordance with apparent porosity increase. Portland cement concrete after two months lost 20% of mass.
Кључне речи:
Sulfur concrete / Fillers / Durability / Mechanical strength / PorosityИзвор:
Construction and Building Materials, 2011, 25, 10, 3926-3934Издавач:
- Elsevier Sci Ltd, Oxford
Финансирање / пројекти:
- Ministry of Science and Technological Development, Republic of Serbia
- Petroleum Industry of Serbia-NIS a.d. Novi [TR 19016]
- Имплементација савременијих техничко-технолошких и еколошких решења у постојећим производним системима Рудника Бакра Бор и Рудника Бакра Мајданпек (RS-MESTD-Technological Development (TD or TR)-33007)
DOI: 10.1016/j.conbuildmat.2011.04.024
ISSN: 0950-0618
WoS: 000292664700017
Scopus: 2-s2.0-79958123359
Институција/група
Tehnološko-metalurški fakultetTY - JOUR AU - Vlahović, Milica M. AU - Martinović, Sanja AU - Boljanac, Tamara AU - Jovanić, Predrag AU - Volkov-Husović, Tatjana PY - 2011 UR - http://TechnoRep.tmf.bg.ac.rs/handle/123456789/1893 AB - Durability of sulfur concrete with different fillers, as well as Portland cement concrete, was tested in the solutions of HCl, H(2)SO(4), and NaCl. Regarding mass changes, in the solutions of HCl and H(2)SO(4) sulfur concrete with talc and fly ash exhibited higher durability, while in NaCl samples with alumina and microsilica were better. The type of filler did not affect durability regarding compressive strength. Strength loss was higher in the solution of HCl comparing to H(2)SO(4), while negligible in NaCl which is in accordance with apparent porosity increase. Portland cement concrete after two months lost 20% of mass. PB - Elsevier Sci Ltd, Oxford T2 - Construction and Building Materials T1 - Durability of sulfur concrete in various aggressive environments EP - 3934 IS - 10 SP - 3926 VL - 25 DO - 10.1016/j.conbuildmat.2011.04.024 ER -
@article{ author = "Vlahović, Milica M. and Martinović, Sanja and Boljanac, Tamara and Jovanić, Predrag and Volkov-Husović, Tatjana", year = "2011", abstract = "Durability of sulfur concrete with different fillers, as well as Portland cement concrete, was tested in the solutions of HCl, H(2)SO(4), and NaCl. Regarding mass changes, in the solutions of HCl and H(2)SO(4) sulfur concrete with talc and fly ash exhibited higher durability, while in NaCl samples with alumina and microsilica were better. The type of filler did not affect durability regarding compressive strength. Strength loss was higher in the solution of HCl comparing to H(2)SO(4), while negligible in NaCl which is in accordance with apparent porosity increase. Portland cement concrete after two months lost 20% of mass.", publisher = "Elsevier Sci Ltd, Oxford", journal = "Construction and Building Materials", title = "Durability of sulfur concrete in various aggressive environments", pages = "3934-3926", number = "10", volume = "25", doi = "10.1016/j.conbuildmat.2011.04.024" }
Vlahović, M. M., Martinović, S., Boljanac, T., Jovanić, P.,& Volkov-Husović, T.. (2011). Durability of sulfur concrete in various aggressive environments. in Construction and Building Materials Elsevier Sci Ltd, Oxford., 25(10), 3926-3934. https://doi.org/10.1016/j.conbuildmat.2011.04.024
Vlahović MM, Martinović S, Boljanac T, Jovanić P, Volkov-Husović T. Durability of sulfur concrete in various aggressive environments. in Construction and Building Materials. 2011;25(10):3926-3934. doi:10.1016/j.conbuildmat.2011.04.024 .
Vlahović, Milica M., Martinović, Sanja, Boljanac, Tamara, Jovanić, Predrag, Volkov-Husović, Tatjana, "Durability of sulfur concrete in various aggressive environments" in Construction and Building Materials, 25, no. 10 (2011):3926-3934, https://doi.org/10.1016/j.conbuildmat.2011.04.024 . .