Photocatalytic Degradation of Bisphenol A with alpha-Fe2O3 Fibers and Particles
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2019)
Two-step synthesis of Fe2O3 particles, performed by precipitation from iron(III) chloride (FeCl3 center dot 6H(2)O) using ammonium hydroxide in first step and calcination at 400 and 700 degrees C during 4 h, provided Fe2O3 ...
Final Flotation Waste Kinetics of Sintering at Different Heating Regimes
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2016)
In the copper extraction, especially during the process of flotation enrichment and the pyrometallurgical processing, the waste materials that represent huge polluters of environment are being generated. In order to examine ...
Sintered materials based on copper and alumina powders synthesized by a novel method
(International Institute for the Science of Sintering, Beograd, 2010)
This paper presents the production of sintered materials from nano-composite powders obtained by a novel synthesis method, which represents a combination of thermochemical synthesis and mechanical alloying. Produced powders ...
Structure and photocatalytic properties of sintered TiO2 nanotube arrays
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2018)
One-dimensional (1D) TiO2 nanotubes perpendicular to the substrate were obtained by electrochemical oxidation of titanium foil in an acid electrolyte. In order to alter the crystallinity and the morphology of films the ...
Anisotropy Analysis of Low Cement Concrete by Ultrasonic Measurements and Image Analysis
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2016)
The analized material was high alumina low cement castable sintered at three different temperatures. Influence of initial material anisotropy on the thermal shock resistance as well as changes of anisotropy level during ...
Solid state synthesis of extra phase-pure Li4Ti5O12 spinel
(Belgrade : International Institute for the Science of Sintering, 2011)
Extra phase-pure Li4Ti5O12 spinel with particle sizes less than 500 nm was synthesized by solid state reaction of mechanochemicaly activated mixture of nano anatase and Li2CO3 for a very short annealing time, 4 h at 800°C. ...
Comparison of Mechanical Behavior of SiC Sintered Specimen to Analysis of Surface Defects
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2014)
Silicon carbide is the material that in sintered form is suiTab. for protection from impact as part of the multilayered structure. Its role is to accumulate energy from the projectile, to plastically deform the projectile ...
Modeling of the Mechanical Behavior of Fiber-Reinforced Ceramic Composites Using Finite Element Method (FEM)
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2014)
Modeling of the mechanical behavior of fiber-reinforced ceramic matrix composites (CMC) is presented by the example of Al2O3 fibers in an alumina based matrix. The starting point of the modeling is a substructure (elementary ...
The Mechanisms of Cavitation Erosion of Raw and Sintered Basalt
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2019)
The paper analyzes the morphology of cavitation damage of raw and sintered basalt samples. The experiment was conducted using the ultrasonic vibratory cavitation test method according to the ASTM G-32 standard. During the ...
Properties of Zig-Zag Nickel Nanostructures Obtained by GLAD Technique
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2016)
Zig-zag structure of the nickel thin film has been obtained using Glancing Angle Deposition (GLAD) technique. Glass substrate was positioned 75 degrees with respect to the substrate normal. The obtained nickel thin film ...