Microstructural properties and cavitation behavior of hypereutectic Al-Si alloy obtained by rheocasting process / Mikrostrukturna svojstva i kavitaciono ponašanje nadeutektičke Al-Si legure dobijene reokasting postupkom
(Engineering Society for Corrosion, Belgrade, Serbia, 2014)
The purpose of this study was to investigate possible application of AlSi alloy produced by rheocasting process in cavitation conditions. A rheocasting process was used to refine the as cast microstructure and improve the ...
Influence of the structural changes on cavitation resistance of Al18SiCuMg alloy produced by rheocasting process / Uticaj strukturnih promena na kavitacionu otpornost Al18SiCuMg legure proizvedene reokasting procesom
(Engineering Society for Corrosion, Belgrade, Serbia, 2015)
The influence of stirring speeds of 1000 and 1500 r/min on the microstructure of Al18SiCuMg alloy was investigated. The smaller size of Si particles of rheocast sample obtained by higher cooling rate and higher stirring ...
Characterisation of biocompatible layers of ZrO28%Y2O used in combination with other ceramics to modify the surface of implants / Karakterizacija biokompatibilnih slojeva ZrO28%Y2O3 koji se koriste u kombinaciji sa drugom keramikom za modifikaciju površine implantata
(Inženjersko društvo za koroziju, 2021)
The aim of this study was to deposit multi-functional ZrO28%Y2O3 coating layers using the plasma spray technology and then to characterise such layers. In combination with other biomedical ceramics, this coating is intended ...
Characterization of plasma spray bioinert coating Al2O328wt.%MgO / Karakterizacija plazma sprej bioinertne prevlake Al2O328tež.%MgO
(Engineering Society for Corrosion, Belgrade, Serbia, 2019)
This paper presents the results of testing mechanical and structural characteristics of plasma spray coating Al2O328wt.%MgO. Metal oxide MgO in a complex oxide Al2O328wt.%MgO modifies the properties of Al2O3 ceramics by ...
Characterization of vacuum plasma spray VPS - W coating deposited on stainless steel substrates / Karakterizacija vakuum plazma sprej VPS - W prevlake deponovane na čeličnim podloga
(Inženjersko društvo za koroziju, 2021)
In this paper, studied was the melting of W powder particles in plasma, their behavior at oxidation as well as the mechanism of hardening on the surface of the substrate. Tungsten coating layers were deposited with vacuum ...
Mechanical properties and microstructure of the ZrO25CaO/NiCrAl coating system / Mehaničke osobine i mikrostruktura sistema prevlaka ZrO25CaO/NiCrAl
(Engineering Society for Corrosion, Belgrade, Serbia, 2019)
ZrO25CaO is a versatile class of material that can be sintered or plasma spray deposited in combination with other materials on the implant substrate. Due to brittleness the organic ceramic hydroxyapatite Ca10(PO4)6(OH)2 ...
Characterization of NiAl layers deposited by atmospheric plasma spray (APS) / Karakterizacija NiAl slojeva deponovanih atmosferskim plazma sprejom (APS)
(Engineering Society for Corrosion, Belgrade, Serbia, 2020)
In this paper analyzed were the mechanical properties and microstructure of the Ni30Al coating layers deposited using atmospheric plasma spray (APS). For deposition of the coating applied was a composite Ni30wt.% Al powder, ...
Mechanical properties and microstructure of molybdenum coating layers deposited vacuum plasma spray process / Mehanička svojstva i mikrostruktura slojeva prevlake molibdena deponovane vakuum plazma sprej procesom
(Engineering Society for Corrosion, Belgrade, Serbia, 2019)
Molybdenum coatings due to their excellent wear resistant properties and sliding characteristics under dry friction conditions are often used in applications to resist friction and dry sliding. Since molybdenum metal is ...
The mechanical and microstructural properties of VPS-Ti porous coating deposited on titanium alloy substrates for osseointegration / Mehanička i mikrostrukturna svojstva VPS-Ti porozne prevlake deponovane na podlogama od legure titana za osteointegraciju
(Engineering Society for Corrosion, Belgrade, Serbia, 2020)
The topography of the surface of the deposited VPS-Ti coatings on substrate surfaces of implants relating to the roughness and porous structure plays a decisive role in the process of on growth of the implants to the bones ...