Show full item recordAbstract
A series of novel thermoplastic elastomers based on ABA-type triblock prepolymers, poly[(propylene oxide)-(dimethylsiloxane)-(propylene oxide)] (PPO-PDMS-PPO), as the soft segments, and poly(butylene terephthalate) (PBT), as the hard segments, was synthesized by catalyzed two-step melt transesterification of dimethyl terephthalate (DMT) with 1,4-butanediol (BD) and α,ω-dihydroxy-(PPO-PDMS-PPO) (M̄ n = 2930 g mol -1 ). Several copolymers with a content of hard PBT segments between 40 and 60 mass% and a constant length of the soft PPO-PDMS-PPO segments were prepared. The siloxane-containing triblock prepolymer with hydrophilic terminal PPO blocks was used to improve the compatibility between the polar comonomers, i.e. DMT and BD, and the non-polar PDMS segments. The structure and composition of the copolymers were examined using 1 H NMR spectroscopy, while the effectiveness of the incorporation of α,ω-dihydroxy-(PPO-PDMS-PPO) prepolymer into the copolyester chains was controlled by chlor...oform extraction. The effect of the structure and composition of the copolymers on the transition temperatures (T m and T g ) and the thermal and thermo-oxidative degradation stability, as well as on the degree of crystallinity, and some rheological properties, were studied.
Keywords:
Poly(ester ether siloxane)s / Thermoplastic elastomers / α-ω-dihydroxy-poly(propyleneoxide-dimethyl-siloxane- propyleneoxide)Source:
Polymer International, 2006, 55, 11, 1304-1314Publisher:
- John Wiley and Sons Ltd
DOI: 10.1002/pi.2085
ISSN: 0959-8103
WoS: 000241203400016
Scopus: 2-s2.0-33750137403
Institution/Community
Tehnološko-metalurški fakultetTY - JOUR AU - Vučković, Marija V. AU - Antić, Vesna V. AU - Dojčinović, Biljana P. AU - Govedarica, Milutin N. AU - Đonlagić, Jasna PY - 2006 UR - http://TechnoRep.tmf.bg.ac.rs/handle/123456789/5472 AB - A series of novel thermoplastic elastomers based on ABA-type triblock prepolymers, poly[(propylene oxide)-(dimethylsiloxane)-(propylene oxide)] (PPO-PDMS-PPO), as the soft segments, and poly(butylene terephthalate) (PBT), as the hard segments, was synthesized by catalyzed two-step melt transesterification of dimethyl terephthalate (DMT) with 1,4-butanediol (BD) and α,ω-dihydroxy-(PPO-PDMS-PPO) (M̄ n = 2930 g mol -1 ). Several copolymers with a content of hard PBT segments between 40 and 60 mass% and a constant length of the soft PPO-PDMS-PPO segments were prepared. The siloxane-containing triblock prepolymer with hydrophilic terminal PPO blocks was used to improve the compatibility between the polar comonomers, i.e. DMT and BD, and the non-polar PDMS segments. The structure and composition of the copolymers were examined using 1 H NMR spectroscopy, while the effectiveness of the incorporation of α,ω-dihydroxy-(PPO-PDMS-PPO) prepolymer into the copolyester chains was controlled by chloroform extraction. The effect of the structure and composition of the copolymers on the transition temperatures (T m and T g ) and the thermal and thermo-oxidative degradation stability, as well as on the degree of crystallinity, and some rheological properties, were studied. PB - John Wiley and Sons Ltd T2 - Polymer International T1 - Synthesis and characterization of poly(ester ether siloxane)s EP - 1314 IS - 11 SP - 1304 VL - 55 DO - 10.1002/pi.2085 ER -
@article{ author = "Vučković, Marija V. and Antić, Vesna V. and Dojčinović, Biljana P. and Govedarica, Milutin N. and Đonlagić, Jasna", year = "2006", abstract = "A series of novel thermoplastic elastomers based on ABA-type triblock prepolymers, poly[(propylene oxide)-(dimethylsiloxane)-(propylene oxide)] (PPO-PDMS-PPO), as the soft segments, and poly(butylene terephthalate) (PBT), as the hard segments, was synthesized by catalyzed two-step melt transesterification of dimethyl terephthalate (DMT) with 1,4-butanediol (BD) and α,ω-dihydroxy-(PPO-PDMS-PPO) (M̄ n = 2930 g mol -1 ). Several copolymers with a content of hard PBT segments between 40 and 60 mass% and a constant length of the soft PPO-PDMS-PPO segments were prepared. The siloxane-containing triblock prepolymer with hydrophilic terminal PPO blocks was used to improve the compatibility between the polar comonomers, i.e. DMT and BD, and the non-polar PDMS segments. The structure and composition of the copolymers were examined using 1 H NMR spectroscopy, while the effectiveness of the incorporation of α,ω-dihydroxy-(PPO-PDMS-PPO) prepolymer into the copolyester chains was controlled by chloroform extraction. The effect of the structure and composition of the copolymers on the transition temperatures (T m and T g ) and the thermal and thermo-oxidative degradation stability, as well as on the degree of crystallinity, and some rheological properties, were studied.", publisher = "John Wiley and Sons Ltd", journal = "Polymer International", title = "Synthesis and characterization of poly(ester ether siloxane)s", pages = "1314-1304", number = "11", volume = "55", doi = "10.1002/pi.2085" }
Vučković, M. V., Antić, V. V., Dojčinović, B. P., Govedarica, M. N.,& Đonlagić, J.. (2006). Synthesis and characterization of poly(ester ether siloxane)s. in Polymer International John Wiley and Sons Ltd., 55(11), 1304-1314. https://doi.org/10.1002/pi.2085
Vučković MV, Antić VV, Dojčinović BP, Govedarica MN, Đonlagić J. Synthesis and characterization of poly(ester ether siloxane)s. in Polymer International. 2006;55(11):1304-1314. doi:10.1002/pi.2085 .
Vučković, Marija V., Antić, Vesna V., Dojčinović, Biljana P., Govedarica, Milutin N., Đonlagić, Jasna, "Synthesis and characterization of poly(ester ether siloxane)s" in Polymer International, 55, no. 11 (2006):1304-1314, https://doi.org/10.1002/pi.2085 . .