Influence of the structural changes on cavitation resistance of Al18SiCuMg alloy produced by rheocasting process / Uticaj strukturnih promena na kavitacionu otpornost Al18SiCuMg legure proizvedene reokasting procesom
(Engineering Society for Corrosion, Belgrade, Serbia, 2015)
The influence of stirring speeds of 1000 and 1500 r/min on the microstructure of Al18SiCuMg alloy was investigated. The smaller size of Si particles of rheocast sample obtained by higher cooling rate and higher stirring ...
Microstructural properties and cavitation behavior of hypereutectic Al-Si alloy obtained by rheocasting process / Mikrostrukturna svojstva i kavitaciono ponašanje nadeutektičke Al-Si legure dobijene reokasting postupkom
(Engineering Society for Corrosion, Belgrade, Serbia, 2014)
The purpose of this study was to investigate possible application of AlSi alloy produced by rheocasting process in cavitation conditions. A rheocasting process was used to refine the as cast microstructure and improve the ...