dc.description.abstractThe influence of hydrogenation on the biocompatibility of different hydroxyapatite (HAP) materials was tested. Materials consisted of pure HAP, HAP substituted with manganese (Mn+2) and with magnesium (Mg+2) - all axially pressed and conventionally sintered for 2 h at 1200 degrees C; pure HAP isostatic pressed and sintered by a microwave technique for 15 min at temperature of 1200 degrees C. Biocompatibility was compared by enumeration of the number of osteoblast-like cells to the materials before and after hydrogenation. Obtained results show that the osteoblastic cells demonstrated a higher ability to attach to HAP if its surface was negatively charged. Hydrogenation altered the surface potential; HAP substituted with manganese - HAP(Mn) and with magnesium - HAP(Mg) demonstrated the highest ability to engineer the charge.en
dc.publisherIOP Publishing Ltd, Bristol
dc.rightsrestrictedAccess
dc.sourceAnnual Conference on Functional Materials and Nanotechnologies - FM&NT 2011
dc.titleThe Influence of Surface Treatment by Hydrogenation on the Biocompatibility of Different Hydroxyapatite Materialsen
dc.typearticle
dc.rights.licenseARR
dc.citation.other23: -
dc.citation.volume23
dc.identifier.doi10.1088/1757-899X/23/1/012032
dc.identifier.scopus2-s2.0-80052019700
dc.identifier.wos000310956600032
dc.type.versionpublishedVersion


Документи

Thumbnail

Овај документ се појављује у следећим колекцијама

Приказ основних података о документу