Durability of sulfur concrete in various aggressive environments
Samo za registrovane korisnike
2011
Autori
Vlahović, Milica M.Martinović, Sanja
Boljanac, Tamara
Jovanić, Predrag
Volkov-Husović, Tatjana
Članak u časopisu (Objavljena verzija)
Metapodaci
Prikaz svih podataka o dokumentuApstrakt
Durability of sulfur concrete with different fillers, as well as Portland cement concrete, was tested in the solutions of HCl, H(2)SO(4), and NaCl. Regarding mass changes, in the solutions of HCl and H(2)SO(4) sulfur concrete with talc and fly ash exhibited higher durability, while in NaCl samples with alumina and microsilica were better. The type of filler did not affect durability regarding compressive strength. Strength loss was higher in the solution of HCl comparing to H(2)SO(4), while negligible in NaCl which is in accordance with apparent porosity increase. Portland cement concrete after two months lost 20% of mass.
Ključne reči:
Sulfur concrete / Fillers / Durability / Mechanical strength / PorosityIzvor:
Construction and Building Materials, 2011, 25, 10, 3926-3934Izdavač:
- Elsevier Sci Ltd, Oxford
Finansiranje / projekti:
- Ministry of Science and Technological Development, Republic of Serbia
- Petroleum Industry of Serbia-NIS a.d. Novi [TR 19016]
- Implementacija savremenijih tehničko-tehnoloških i ekoloških rešenja u postojećim proizvodnim sistemima Rudnika Bakra Bor i Rudnika Bakra Majdanpek (RS-MESTD-Technological Development (TD or TR)-33007)
DOI: 10.1016/j.conbuildmat.2011.04.024
ISSN: 0950-0618
WoS: 000292664700017
Scopus: 2-s2.0-79958123359
Institucija/grupa
Tehnološko-metalurški fakultetTY - JOUR AU - Vlahović, Milica M. AU - Martinović, Sanja AU - Boljanac, Tamara AU - Jovanić, Predrag AU - Volkov-Husović, Tatjana PY - 2011 UR - http://TechnoRep.tmf.bg.ac.rs/handle/123456789/1893 AB - Durability of sulfur concrete with different fillers, as well as Portland cement concrete, was tested in the solutions of HCl, H(2)SO(4), and NaCl. Regarding mass changes, in the solutions of HCl and H(2)SO(4) sulfur concrete with talc and fly ash exhibited higher durability, while in NaCl samples with alumina and microsilica were better. The type of filler did not affect durability regarding compressive strength. Strength loss was higher in the solution of HCl comparing to H(2)SO(4), while negligible in NaCl which is in accordance with apparent porosity increase. Portland cement concrete after two months lost 20% of mass. PB - Elsevier Sci Ltd, Oxford T2 - Construction and Building Materials T1 - Durability of sulfur concrete in various aggressive environments EP - 3934 IS - 10 SP - 3926 VL - 25 DO - 10.1016/j.conbuildmat.2011.04.024 ER -
@article{ author = "Vlahović, Milica M. and Martinović, Sanja and Boljanac, Tamara and Jovanić, Predrag and Volkov-Husović, Tatjana", year = "2011", abstract = "Durability of sulfur concrete with different fillers, as well as Portland cement concrete, was tested in the solutions of HCl, H(2)SO(4), and NaCl. Regarding mass changes, in the solutions of HCl and H(2)SO(4) sulfur concrete with talc and fly ash exhibited higher durability, while in NaCl samples with alumina and microsilica were better. The type of filler did not affect durability regarding compressive strength. Strength loss was higher in the solution of HCl comparing to H(2)SO(4), while negligible in NaCl which is in accordance with apparent porosity increase. Portland cement concrete after two months lost 20% of mass.", publisher = "Elsevier Sci Ltd, Oxford", journal = "Construction and Building Materials", title = "Durability of sulfur concrete in various aggressive environments", pages = "3934-3926", number = "10", volume = "25", doi = "10.1016/j.conbuildmat.2011.04.024" }
Vlahović, M. M., Martinović, S., Boljanac, T., Jovanić, P.,& Volkov-Husović, T.. (2011). Durability of sulfur concrete in various aggressive environments. in Construction and Building Materials Elsevier Sci Ltd, Oxford., 25(10), 3926-3934. https://doi.org/10.1016/j.conbuildmat.2011.04.024
Vlahović MM, Martinović S, Boljanac T, Jovanić P, Volkov-Husović T. Durability of sulfur concrete in various aggressive environments. in Construction and Building Materials. 2011;25(10):3926-3934. doi:10.1016/j.conbuildmat.2011.04.024 .
Vlahović, Milica M., Martinović, Sanja, Boljanac, Tamara, Jovanić, Predrag, Volkov-Husović, Tatjana, "Durability of sulfur concrete in various aggressive environments" in Construction and Building Materials, 25, no. 10 (2011):3926-3934, https://doi.org/10.1016/j.conbuildmat.2011.04.024 . .