dc.description.abstractThe results of the investigation of the reduction degree on the hardness of a gold sample with chemical composition Au58,5Ag15Cu9,5Ni9Zn5Pd3 for old white gold alloy and Au58,5Ag18Cu10,5Ga8Zn5 (wt %) for new white gold alloy, are shown. The obtained results show that hardness of samples is higher when total reduction is higher, and that it decreases after process annealing. Also, the mechanical properties of the investigated alloys were compared. Alloy without Ni has lower hardness and higher elongation values.en
dc.publisherBulgarian Acad Science, Sofia
dc.relationinfo:eu-repo/grantAgreement/MESTD/MPN2006-2010/19018/RS//
dc.rightsrestrictedAccess
dc.sourceBulgarian Chemical Communications
dc.subjectwhite golden
dc.subjectrollingen
dc.subjectdrawingen
dc.subjecthardnessen
dc.subjecttotal elongationen
dc.subjectnickelen
dc.subjectgalliumen
dc.titleDifferences in the mode of thermomechanical processing between white gold alloys to produce semi-finished productsen
dc.typearticle
dc.rights.licenseARR
dc.citation.epage166
dc.citation.issue1
dc.citation.other47(1): 161-166
dc.citation.rankM23
dc.citation.spage161
dc.citation.volume47
dc.identifier.rcubhttps://hdl.handle.net/21.15107/rcub_technorep_3089
dc.identifier.wos000367650000025
dc.type.versionpublishedVersion


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record