Final Flotation Waste Kinetics of Sintering at Different Heating Regimes
2016
Autori
Cocić, MiraLogar, Mihovil
Matović, Branko
Dević, Snežana
Volkov-Husović, Tatjana
Cocić, Sasa
Tasić, Visa
Članak u časopisu (Objavljena verzija)
Metapodaci
Prikaz svih podataka o dokumentuApstrakt
In the copper extraction, especially during the process of flotation enrichment and the pyrometallurgical processing, the waste materials that represent huge polluters of environment are being generated. In order to examine the application of Final flotation waste (FFW) in the manufacturing of new materials from the glass-ceramic group phase and mineral composition were examined as well as thermal properties. FFW kinetics of sintering has been tested at different dyamics (1 degrees C/min, 29 degrees C/min and 43 degrees C/min), in order to find the optimum conditions for sintering with a minimum amount of energy and time consumption. The samples were examined using: X-ray diffraction, X-ray fluorescence analysis, SEM (Scanning Electron Microscopy) and thermal microscopy. The best results for the production of glass ceramic materials were obtained during the sintering at heating regime of 29 degrees C/min.
Ključne reči:
Final flotation waste / Kinetics of sintering / Heating rate / Particle size distribution / Glass ceramicsIzvor:
Science of Sintering, 2016, 48, 2, 197-208Izdavač:
- Međunarodni Institut za nauku o sinterovanju, Beograd
Finansiranje / projekti:
- Minerali Srbije: sastav, struktura, geneza, primena i doprinos održanju životne sredine (RS-MESTD-Basic Research (BR or ON)-176010)
DOI: 10.2298/SOS1602197C
ISSN: 0350-820X
WoS: 000382653600007
Scopus: 2-s2.0-84994639505
Institucija/grupa
Tehnološko-metalurški fakultetTY - JOUR AU - Cocić, Mira AU - Logar, Mihovil AU - Matović, Branko AU - Dević, Snežana AU - Volkov-Husović, Tatjana AU - Cocić, Sasa AU - Tasić, Visa PY - 2016 UR - http://TechnoRep.tmf.bg.ac.rs/handle/123456789/3341 AB - In the copper extraction, especially during the process of flotation enrichment and the pyrometallurgical processing, the waste materials that represent huge polluters of environment are being generated. In order to examine the application of Final flotation waste (FFW) in the manufacturing of new materials from the glass-ceramic group phase and mineral composition were examined as well as thermal properties. FFW kinetics of sintering has been tested at different dyamics (1 degrees C/min, 29 degrees C/min and 43 degrees C/min), in order to find the optimum conditions for sintering with a minimum amount of energy and time consumption. The samples were examined using: X-ray diffraction, X-ray fluorescence analysis, SEM (Scanning Electron Microscopy) and thermal microscopy. The best results for the production of glass ceramic materials were obtained during the sintering at heating regime of 29 degrees C/min. PB - Međunarodni Institut za nauku o sinterovanju, Beograd T2 - Science of Sintering T1 - Final Flotation Waste Kinetics of Sintering at Different Heating Regimes EP - 208 IS - 2 SP - 197 VL - 48 DO - 10.2298/SOS1602197C ER -
@article{ author = "Cocić, Mira and Logar, Mihovil and Matović, Branko and Dević, Snežana and Volkov-Husović, Tatjana and Cocić, Sasa and Tasić, Visa", year = "2016", abstract = "In the copper extraction, especially during the process of flotation enrichment and the pyrometallurgical processing, the waste materials that represent huge polluters of environment are being generated. In order to examine the application of Final flotation waste (FFW) in the manufacturing of new materials from the glass-ceramic group phase and mineral composition were examined as well as thermal properties. FFW kinetics of sintering has been tested at different dyamics (1 degrees C/min, 29 degrees C/min and 43 degrees C/min), in order to find the optimum conditions for sintering with a minimum amount of energy and time consumption. The samples were examined using: X-ray diffraction, X-ray fluorescence analysis, SEM (Scanning Electron Microscopy) and thermal microscopy. The best results for the production of glass ceramic materials were obtained during the sintering at heating regime of 29 degrees C/min.", publisher = "Međunarodni Institut za nauku o sinterovanju, Beograd", journal = "Science of Sintering", title = "Final Flotation Waste Kinetics of Sintering at Different Heating Regimes", pages = "208-197", number = "2", volume = "48", doi = "10.2298/SOS1602197C" }
Cocić, M., Logar, M., Matović, B., Dević, S., Volkov-Husović, T., Cocić, S.,& Tasić, V.. (2016). Final Flotation Waste Kinetics of Sintering at Different Heating Regimes. in Science of Sintering Međunarodni Institut za nauku o sinterovanju, Beograd., 48(2), 197-208. https://doi.org/10.2298/SOS1602197C
Cocić M, Logar M, Matović B, Dević S, Volkov-Husović T, Cocić S, Tasić V. Final Flotation Waste Kinetics of Sintering at Different Heating Regimes. in Science of Sintering. 2016;48(2):197-208. doi:10.2298/SOS1602197C .
Cocić, Mira, Logar, Mihovil, Matović, Branko, Dević, Snežana, Volkov-Husović, Tatjana, Cocić, Sasa, Tasić, Visa, "Final Flotation Waste Kinetics of Sintering at Different Heating Regimes" in Science of Sintering, 48, no. 2 (2016):197-208, https://doi.org/10.2298/SOS1602197C . .