Претраживање
Приказ резултата 1-10 од 1015
Crack propagation in 3PB specimen made from welded joint
(1st Virtual European Conference on Fracture - Vecf1, 2020)
Crack propagation in 3PB specimen has been investigated experimentally by using Digital Image Correlation (DIC) technique. For this purpose, specimens were taken from butt welded plates, made of P460NL1 micro-alloyed steel. ...
The influence of chemical modifications on the chemical composition, sorption properties and volume electrical resistivity of jute fabrics / Uticaj hemijskog modifikovanja tkanine jute na promenu hemijskog sastava, sorpcionih svojstava i specifične zapreminske električne otpornosti
(Belgrade : Union of Engineers and Technicians of Serbia, 2018)
The influence of chemical modifications on chemical composition, sorption properties and volume electrical resistivity of jute fabrics was studied, In order to partially remove hemicelluloses and lignin, modifications with ...
The analysis of forming PVB-SiO2 nanocomposite fibers by the electrospinning process / Analiza formiranja PVB-SiO2 nanokompozitnih vlakana pomoću elektrospining procesa
(Military Technical Institute, Belgrade, 2011)
The poly (vinyl butyral)-silica (PVB-SiO2) nanofibers were obtained by the electrospinning process. The experiments were carried out with PVB solution in concentration of 10 wt.% where ethanol was used as the solvent. The ...
Hydroxyapatite/nifuroxazide conjugate: Characterization, drug release and antimicrobial activity / Хидроксиапатит/нифуроксазид конјугат: карактеризација, отпуштање лека и антимикробна активност
(Serbian Chemical Society, 2021)
Synthetic hydroxyapatite (Ca-10(PO4)(6)(OH)(2), HAp) is very similar to the inorganic part of the bones and teeth of mammals. It is a well-known biomaterial with good biocompatibility, osteoconductivity and bioactivity. ...
Sitting position awake craniostomy with drainage for chronic subdural hematoma: a viable alternative?
(Vojnosanitetski Pregled, 2021)
Background/Aim. Chronic subdural hematoma (CSDH) is one of the most frequent neurosurgical conditions with an overall incidence ranging from 1.72 to 20.6 per 100,000 persons per year. The surgical procedure for CSDH is ...
Corrosion Stability of Corrosion Products on an Archaeological Iron Artefact
(Alexandru Ioan Cuza University Publiching House Iasi-Romania, 2012)
A spearhead of archaeological and cultural significance has been found and analysed in
Serbia. In the corrosion products of the artefact, the dominant phases were goethite (α-
FeO(OH)) and magnetite (Fe3O4) whose presence ...
Controlled swelling and degradation studies of alginate microbeads in dilute natrium citrate solutions / Ispitivanje mogućnosti kontrolisanog bubrenja i razgradnje alginatnih mikročestica u razblaženim rastvorima natrijum-citrata
(Association of Chemical Engineers of Serbia, 2010)
Alginate hydrogels are widely used in biomedicine due to alginate availability, hydrophilic nature, biocompatibility and biodegradability. Alginate microbeads are particularly attractive for applications in pharmacy and ...
Micro Nanofibrillated Cellulose as Functional Additive Supporting Processability of Surface-Active Mineral Suspensions: Exemplified by Pixel Coating of an NOx-Sorbent Layer
(MDPI, 2023)
Unlike established coating formulations, functional particulate coatings often demand the omission of polymer dispersant so as to retain surface functionality. This results in heterogeneous complex rheology. We take an ...
Influence of N doping on structural and photocatalytic properties of hydrothermally synthesized TiO2/carbon composites
(Journal of the Serbian Chemical Society, 2023)
Abstract: N-doped TiO2/carbon composites (TiO2/CN) with different nitrogen content, were obtained starting from titanium isopropoxide and glucose, and by varying the amount of melamine, added to starting reaction mixture. ...
Naponska korozija metala i legura i njihovih zavarenih spojeva, Deo I: uslovi nastanka naponske korozije
(DUZS - Društvo za unapređivanje zavarivanja u Srbiji, Beograd, Srbija, 2012)
Opisani su osnovni mehanizmi naponske korozije različitih metala i legura i njihovih zavarenih spojeva. Detaljnije su
razmotreni metalurški i korozioni uslovi nastanka naponske korozije ugljeničnih i niskolegiranih čelika, ...