Претраживање
Приказ резултата 1-10 од 13
Characterization of vacuum plasma spray VPS - W coating deposited on stainless steel substrates / Karakterizacija vakuum plazma sprej VPS - W prevlake deponovane na čeličnim podloga
(Inženjersko društvo za koroziju, 2021)
In this paper, studied was the melting of W powder particles in plasma, their behavior at oxidation as well as the mechanism of hardening on the surface of the substrate. Tungsten coating layers were deposited with vacuum ...
Optimizing the content of nickel in flux-cored wire intended for welding micro-alloyed steels / Optimizacija sadržaja nikla u punjenoj žici namenjenoj za zavarivanje mikrolegiranih čelika
(DUZS - Društvo za unapređivanje zavarivanja u Srbiji, Beograd, 2014)
This paper presents the results related to organizing production of flux-cored wire alloyed with Ni and Mo according to standard AWS A5.29 intended for the MAG welding process. On the experimental line for steel strip ...
The mechanical and microstructural properties of VPS-Ti porous coating deposited on titanium alloy substrates for osseointegration / Mehanička i mikrostrukturna svojstva VPS-Ti porozne prevlake deponovane na podlogama od legure titana za osteointegraciju
(Engineering Society for Corrosion, Belgrade, Serbia, 2020)
The topography of the surface of the deposited VPS-Ti coatings on substrate surfaces of implants relating to the roughness and porous structure plays a decisive role in the process of on growth of the implants to the bones ...
Characterization of plasma spray bioinert coating Al2O328wt.%MgO / Karakterizacija plazma sprej bioinertne prevlake Al2O328tež.%MgO
(Engineering Society for Corrosion, Belgrade, Serbia, 2019)
This paper presents the results of testing mechanical and structural characteristics of plasma spray coating Al2O328wt.%MgO. Metal oxide MgO in a complex oxide Al2O328wt.%MgO modifies the properties of Al2O3 ceramics by ...
Mechanical properties and microstructure of the ZrO25CaO/NiCrAl coating system / Mehaničke osobine i mikrostruktura sistema prevlaka ZrO25CaO/NiCrAl
(Engineering Society for Corrosion, Belgrade, Serbia, 2019)
ZrO25CaO is a versatile class of material that can be sintered or plasma spray deposited in combination with other materials on the implant substrate. Due to brittleness the organic ceramic hydroxyapatite Ca10(PO4)6(OH)2 ...
Mechanical properties and microstructure of molybdenum coating layers deposited vacuum plasma spray process / Mehanička svojstva i mikrostruktura slojeva prevlake molibdena deponovane vakuum plazma sprej procesom
(Engineering Society for Corrosion, Belgrade, Serbia, 2019)
Molybdenum coatings due to their excellent wear resistant properties and sliding characteristics under dry friction conditions are often used in applications to resist friction and dry sliding. Since molybdenum metal is ...
INTEGRITY AND RISK ASSESSMENT OF RECONSTRUCTED STEAM LINE / PROCENA INTEGRITETA I RIZIKA REKONSTRUISANOG PAROVODA
(Society for Structural Integrity and Life (DIVK), 2023)
The integrity assessment of high pressure steam pipeline
primarily requires stress state determination, including not
only effects of working pressure and temperature, but also
all acting loads. Toward this aim, the ...
Characterization of NiAl layers deposited by atmospheric plasma spray (APS) / Karakterizacija NiAl slojeva deponovanih atmosferskim plazma sprejom (APS)
(Engineering Society for Corrosion, Belgrade, Serbia, 2020)
In this paper analyzed were the mechanical properties and microstructure of the Ni30Al coating layers deposited using atmospheric plasma spray (APS). For deposition of the coating applied was a composite Ni30wt.% Al powder, ...
Characterisation of biocompatible layers of ZrO28%Y2O used in combination with other ceramics to modify the surface of implants / Karakterizacija biokompatibilnih slojeva ZrO28%Y2O3 koji se koriste u kombinaciji sa drugom keramikom za modifikaciju površine implantata
(Inženjersko društvo za koroziju, 2021)
The aim of this study was to deposit multi-functional ZrO28%Y2O3 coating layers using the plasma spray technology and then to characterise such layers. In combination with other biomedical ceramics, this coating is intended ...
Investigation of thermodynamic properties and phase equilibria in Ag-In-Sn system / Ispitivanje termodinamičkih veličina i faznih ravnoteža u sistemu Ag-In-Sn
(Savez inženjera i tehničara Srbije, Beograd, 2006)
Lead - free soldering became very popular in the whole world, because of high ecological demands in industry. Most of alternative alloys have high content of tin, and some of them are already used in electronic industry. ...