dc.description.abstractA cost-effective and simple hydrometallurgy procedure for recycling the diamond core drilling crowns by nitric acid leaching, followed by the sodium hydroxide leaching, has been developed. The effect of temperature, nitric acid/sodium hydroxide concentration, leaching time and stirring rate were studied. For the acid leaching process the optimal values for parameters were 60 degrees C, 1.0 M HNO3, 2.5 h, and 800 rpm. It has been noted that the key factors in the alkaline leaching process were temperature and NaOH concentration. For the alkaline leaching, the optimal parameters were 100 degrees C, 40% concentration of NaOH solution, and leaching time of 4 h. Identification and characterisation of products in all technological processes were performed by X-Ray Diffraction (XRD), scanning electron microscope using energy-dispersive X-ray spectroscopy (SEM-EDS), and laser desorption ionisation mass spectrometry (LDI-MS). The analysis of solutions in all phases was performed by inductively coupled plasma atomic emission spectroscopy (ICP-AES). The use of LDI-MS as a new approach to identify the products after phases in the recycling process was an important part of the study, and the results were consistent with the XRD analysis. The total tungsten recovery was over 95.6%, with a high purity of the obtained tungsten trioxide.en
dc.relationinfo:eu-repo/grantAgreement/MESTD/inst-2020/200017/RS//
dc.relationinfo:eu-repo/grantAgreement/MESTD/inst-2020/200135/RS//
dc.relationinfo:eu-repo/grantAgreement/MESTD/inst-2020/200052/RS//
dc.rightsrestrictedAccess
dc.sourceInternational Journal of Refractory Metals & Hard Materials
dc.subjectLDI-MSen
dc.subjectTungsten trioxideen
dc.subjectRecyclingen
dc.subjectDrilling crownsen
dc.subjectHydrometallurgyen
dc.titleRecovery of tungsten trioxide from waste diamond core drilling crowns by nitric acid leachingen
dc.typearticle
dc.rights.licenseARR
dc.citation.other101(): -
dc.citation.rankM21
dc.citation.volume101
dc.identifier.doi10.1016/j.ijrmhm.2021.105695
dc.identifier.scopus2-s2.0-85122655286
dc.identifier.wos000706606300003
dc.type.versionpublishedVersion


Документи

Thumbnail

Овај документ се појављује у следећим колекцијама

Приказ основних података о документу