Strontium titanate thin films were prepared by spray pyrolysis technique. Deposition parameters, such as solution concentration, time and temperature of deposition, and flow rate of carrier gas were optimized to obtain dense films without cracks. Films with different thicknesses were prepared through the control of deposition time. Prepared thin films were homogeneous, well crystallized, with uniform grain size.
Кључне речи:
strontium titanate / sol-gel processes / filmsИзвор:
Journal of the European Ceramic Society, 2004, 24, 6, 989-991Издавач:
- Elsevier Sci Ltd, Oxford
DOI: 10.1016/S0955-2219(03)00459-X
ISSN: 0955-2219
WoS: 000189247800018
Scopus: 2-s2.0-0942289088
Институција/група
Tehnološko-metalurški fakultetTY - JOUR AU - Branković, Goran AU - Branković, Zorica AU - Varela, JA AU - Longo, Elson PY - 2004 UR - http://TechnoRep.tmf.bg.ac.rs/handle/123456789/5414 AB - Strontium titanate thin films were prepared by spray pyrolysis technique. Deposition parameters, such as solution concentration, time and temperature of deposition, and flow rate of carrier gas were optimized to obtain dense films without cracks. Films with different thicknesses were prepared through the control of deposition time. Prepared thin films were homogeneous, well crystallized, with uniform grain size. PB - Elsevier Sci Ltd, Oxford T2 - Journal of the European Ceramic Society T1 - Strontium titanate films prepared by spray pyrolysis EP - 991 IS - 6 SP - 989 VL - 24 DO - 10.1016/S0955-2219(03)00459-X ER -
@article{ author = "Branković, Goran and Branković, Zorica and Varela, JA and Longo, Elson", year = "2004", abstract = "Strontium titanate thin films were prepared by spray pyrolysis technique. Deposition parameters, such as solution concentration, time and temperature of deposition, and flow rate of carrier gas were optimized to obtain dense films without cracks. Films with different thicknesses were prepared through the control of deposition time. Prepared thin films were homogeneous, well crystallized, with uniform grain size.", publisher = "Elsevier Sci Ltd, Oxford", journal = "Journal of the European Ceramic Society", title = "Strontium titanate films prepared by spray pyrolysis", pages = "991-989", number = "6", volume = "24", doi = "10.1016/S0955-2219(03)00459-X" }
Branković, G., Branković, Z., Varela, J.,& Longo, E.. (2004). Strontium titanate films prepared by spray pyrolysis. in Journal of the European Ceramic Society Elsevier Sci Ltd, Oxford., 24(6), 989-991. https://doi.org/10.1016/S0955-2219(03)00459-X
Branković G, Branković Z, Varela J, Longo E. Strontium titanate films prepared by spray pyrolysis. in Journal of the European Ceramic Society. 2004;24(6):989-991. doi:10.1016/S0955-2219(03)00459-X .
Branković, Goran, Branković, Zorica, Varela, JA, Longo, Elson, "Strontium titanate films prepared by spray pyrolysis" in Journal of the European Ceramic Society, 24, no. 6 (2004):989-991, https://doi.org/10.1016/S0955-2219(03)00459-X . .