Corrosion of Archaelogical Artefact made of Forged Iron
Чланак у часопису (Објављена верзија)
Метаподаци
Приказ свих података о документуАпстракт
One artefact of the archaeological cultural heritage from Roman period (IV century) that was
found near Šabac in Serbia, was analysed. In corrosion products of the artefact (knife),
dominant phases were goethite (α-FeOOH) and magnetite (Fe3O4). Presence of these types
of corrosion products explains a good preservation of the base metal (iron) over the centuries
and stability after excavation. Also, the less stable lepidocrocite (γ-FeOOH) and the phases
that come from rocks and land surrounding environment (like SiO2) were identified in the
corrosion products. Phases containing chloride ions (i.e. akaganéite) have not been detected
in the corrosion products. This indirectly indicates that the amount chloride ions were rather
low in underground exploitation conditions.
Кључне речи:
archaeology / iron / corrosion stability / radiography / XRDИзвор:
Metallurgical and Materials Engineering, 2012, 18, 3, 233-240Издавач:
- Savez inženjera matalurgije Srbije, Kneza Miloša 9, 11000 Beograd
Финансирање / пројекти:
- Истраживање и оптимизација технолошких и функционалних перформанси вентилационог млина термоелектране Костолац Б (RS-MESTD-Technological Development (TD or TR)-34028)
Институција/група
Inovacioni centarTY - JOUR AU - Jegdić, Bore V. AU - Polić-Radovanović, Suzana AU - Ristić, Slavica AU - Alil, Ana PY - 2012 UR - http://TechnoRep.tmf.bg.ac.rs/handle/123456789/6232 AB - One artefact of the archaeological cultural heritage from Roman period (IV century) that was found near Šabac in Serbia, was analysed. In corrosion products of the artefact (knife), dominant phases were goethite (α-FeOOH) and magnetite (Fe3O4). Presence of these types of corrosion products explains a good preservation of the base metal (iron) over the centuries and stability after excavation. Also, the less stable lepidocrocite (γ-FeOOH) and the phases that come from rocks and land surrounding environment (like SiO2) were identified in the corrosion products. Phases containing chloride ions (i.e. akaganéite) have not been detected in the corrosion products. This indirectly indicates that the amount chloride ions were rather low in underground exploitation conditions. PB - Savez inženjera matalurgije Srbije, Kneza Miloša 9, 11000 Beograd T2 - Metallurgical and Materials Engineering T1 - Corrosion of Archaelogical Artefact made of Forged Iron EP - 240 IS - 3 SP - 233 VL - 18 UR - https://hdl.handle.net/21.15107/rcub_technorep_6232 ER -
@article{ author = "Jegdić, Bore V. and Polić-Radovanović, Suzana and Ristić, Slavica and Alil, Ana", year = "2012", abstract = "One artefact of the archaeological cultural heritage from Roman period (IV century) that was found near Šabac in Serbia, was analysed. In corrosion products of the artefact (knife), dominant phases were goethite (α-FeOOH) and magnetite (Fe3O4). Presence of these types of corrosion products explains a good preservation of the base metal (iron) over the centuries and stability after excavation. Also, the less stable lepidocrocite (γ-FeOOH) and the phases that come from rocks and land surrounding environment (like SiO2) were identified in the corrosion products. Phases containing chloride ions (i.e. akaganéite) have not been detected in the corrosion products. This indirectly indicates that the amount chloride ions were rather low in underground exploitation conditions.", publisher = "Savez inženjera matalurgije Srbije, Kneza Miloša 9, 11000 Beograd", journal = "Metallurgical and Materials Engineering", title = "Corrosion of Archaelogical Artefact made of Forged Iron", pages = "240-233", number = "3", volume = "18", url = "https://hdl.handle.net/21.15107/rcub_technorep_6232" }
Jegdić, B. V., Polić-Radovanović, S., Ristić, S.,& Alil, A.. (2012). Corrosion of Archaelogical Artefact made of Forged Iron. in Metallurgical and Materials Engineering Savez inženjera matalurgije Srbije, Kneza Miloša 9, 11000 Beograd., 18(3), 233-240. https://hdl.handle.net/21.15107/rcub_technorep_6232
Jegdić BV, Polić-Radovanović S, Ristić S, Alil A. Corrosion of Archaelogical Artefact made of Forged Iron. in Metallurgical and Materials Engineering. 2012;18(3):233-240. https://hdl.handle.net/21.15107/rcub_technorep_6232 .
Jegdić, Bore V., Polić-Radovanović, Suzana, Ristić, Slavica, Alil, Ana, "Corrosion of Archaelogical Artefact made of Forged Iron" in Metallurgical and Materials Engineering, 18, no. 3 (2012):233-240, https://hdl.handle.net/21.15107/rcub_technorep_6232 .