Search
Now showing items 1-6 of 6
Polycrystalline (Y0.7Gd0.3)(2)O-3:Eu3+ ceramics fabricated by Spark Plasma Sintering: Densification and microstructure development
(Elsevier Sci Ltd, Oxford, 2014)
Using Spark Plasma Sintering it is possible to produce polycrystalline ceramics of very fine microstructure and good mechanical properties. This work presents the fabrication of such ceramics using Eu3+-doped (Y0.7Gd0.3)(2)O-3 ...
Absorption boost of TiO2 nanotubes by doping with N and sensitization with CdS quantum dots
(Elsevier Sci Ltd, Oxford, 2017)
A process of obtaining N-doped TiO2 nanotubes sensitized by CdS nanoparticles is presented, including detailed characterizations performed along the synthesis. Transparent TiO2 films consisting of nanotubes, 2.5 mu m long ...
Ex-situ sensitization of ordered TiO2 nanotubes with CdS quantum dots
(Elsevier Sci Ltd, Oxford, 2015)
Ordered titania nanotubes (pore diameter approximate to 90 nm and wall thickness approximate to 10 nm) were obtained by the anodization technique and used for the ex-situ deposition of cadmium sulfide quantum dots (CdS ...
Comparative study of CeO2 nanopowders obtained by the hydrothermal method from various precursors
(Elsevier Sci Ltd, Oxford, 2015)
The effects of common precursors used in the synthesis of CeO2 nanopowders were investigated, and the structural and spectral properties of the resulting products were compared. Two cerium (III) salts, i.e., Ce(NO3)(3)center ...
Dry-pressed anodized titania nanotube/CH3NH3PbI3 single crystal heterojunctions: The beneficial role of N doping
(Elsevier Sci Ltd, Oxford, 2019)
Highly ordered, anodically grown TiO2 nanotubes on titanium supports were annealed in ammonia atmosphere in order to incorporate nitrogen doping ( lt = 2 at.%) in the titanium oxide lattice. FESEM micrographs revealed ...
Nanoindentation study of nickel manganite ceramics obtained by a complex polymerization method
(Elsevier Sci Ltd, Oxford, 2016)
The chemical synthesis of nickel manganite powder was performed by a complex polymerization method (CPM). The obtained fine nanoscaled powders were uniaxially pressed and sintered at different temperatures: 1000-1200 degrees ...