Search
Now showing items 1-10 of 40
Impact of choice of stabilized hysteresis loop on the end result of investigation of high-strength low-alloy (hsla) steel on low cycle fatigue
(Croatian Metallurgical Soc, Zagreb, 2014)
High strength low-alloy steel under low cycle fatigue at a certain level of strain controlled achieve stabilized condition. During the fatigue loading stabilized hysteresis loop is determined, which typical cycle of ...
Effect of surface modified TiO2 nanoparticles on thermal, barrier and mechanical properties of long oil alkyd resin-based coatings
(Budapest Univ Technol & Econ, Budapest, 2015)
Novel soy alkyd-based nanocomposites (NCs) were prepared using TiO2 nanoparticles (NPs) surface modified with different gallates, and for the first time with imine obtained from 3,4-dihydroxybenzaldehyde and oleylamine ...
Dynamic mechanical properties of aramid fabrics impregnated with multiwalled carbon nanotubes / Dinamičko mehanička svojstva aramidnih lamina impregnisanih sa višeslojnim ugljeničnim nanocevima
(Engineering Society for Corrosion, Belgrade, Serbia, 2013)
Carbon nanotubes (CNT) represent allotropes of carbon with a cylindrical nanostructure. In multiwalled carbon nanotubes (MWCNT), graphitic layers make up concentric tubes. The multiwalled nanotubes length in our research ...
Identification of low cycle fatigue parameters of high strength low-alloy (hsla) steel at room temperature
(Croatian Metallurgical Soc, Zagreb, 2014)
Low cycle fatigue test was performed in ambient atmosphere at room temperature. cycle loading of material, in case of High strength low-alloy steel, entails modifications of its properties and in this paper is therefore ...
Effect of hydroxyapatite spheres, whiskers, and nanoparticles on mechanical properties of a model BisGMA/TEGDMA composite initially and after storage
(Wiley-Blackwell, Hoboken, 2013)
This study investigated the effect of shape, size, and surface modification of hydroxyapatite (HAP) fillers on the degree of conversion (DC) and mechanical properties of a model BisGMA/TEGDMA composite initially and after ...
The impact of wood fiber surface modification on physical properties of wood-polymer composites / Uticaj modifikacije površine vlakana drveta na mehanička svojstva kompozita polimer-drvo
(Savez inženjera i tehničara Srbije, Beograd, 2016)
In this paper, the impact of wood fiber surface modification on mechanical properties of poly-(methyl methacrylate)(PMMA)-wood composite was examined. FTIR analysis has shown that the wood fiber surface modification was ...
The effect of calcinated hydroxyapatite and magnesium doped hydroxyapatite as fillers on the mechanical properties of a model bisgma/tegdma dental composite initially and after aging
(Savez inženjera metalurgije Srbije, Beograd, 2018)
This study aimed to investigate the possibility of modifying model BisGMA/TEGDMA dental composite by substituting 10 wt. % of conventional glass fillers with bioactive fillers based on calcinated nanosized hydroxyapatite ...
The effect of friction stirs welding speed on microstructure, mechanical properties and IGC of EN AW-5083 plates
(Advanced Technologies and Materials, 2019)
The aim of this work was to evaluate the influence of welding speed on microstructure, mechanical properties, as well as Intergranular corrosion (IGC) susceptibility of EN AW-5083 alloy welded using FSW. FSW was performed ...
PVB/sepiolite nanocomposites as reinforcement agents for paper
(Srpsko hemijsko društvo, Beograd, 2016)
In order to improve the mechanical properties of paper, 1, 3 and 5 wt. % of sepiolite were dispersed in a poly(vinyl butyral) (PVB) matrix and coated onto the surface of schrenz (110 g m(-2)). Deagglomerated sepiolite ...
Mehanička svojstva hibridnog kompozita UHMWPE/EVA ojačanog vlaknima dobijenim elektropredenjem / Mechanical properties of UHMWPE/EVA hybrid composite reinforced with fibers obtained by electrospinning
(Savez inženjera i tehničara Srbije, 2018)
Aluminijum oksidna (Al2O3) nanovlakna pripremljena su iz vodenog rastvora aluminijum hlorohidrata/poli(vinil alkohola) (PVA) korišćenjem tehnike elektropredenja. Maseni odnos aluminijum hlorohidrata/PVA bio je 5:1. Nakon ...