Претраживање
Приказ резултата 31-40 од 68
Naponska korozija metala i legura i njihovih zavarenih spojeva, Deo II: metode ispitivanja
(DUZS - Društvo za unapređivanje zavarivanja u Srbiji, Beograd, Srbija, 2012)
U radu su razmotrene metode ispitivanja naponske korozije metala i legura i njihovih zavarenih spojeva. Opisani su
principi tih metoda, postupci izvođenja, oblasti primene, kao i prednosti i nedostaci pojedinih metoda. ...
Dynamic mechanical properties of aramid fabrics impregnated with multiwalled carbon nanotubes / Dinamičko mehanička svojstva aramidnih lamina impregnisanih sa višeslojnim ugljeničnim nanocevima
(Engineering Society for Corrosion, Belgrade, Serbia, 2013)
Carbon nanotubes (CNT) represent allotropes of carbon with a cylindrical nanostructure. In multiwalled carbon nanotubes (MWCNT), graphitic layers make up concentric tubes. The multiwalled nanotubes length in our research ...
Naponska korozija metala i legura i njihovih zavarenih spojeva, Deo I: uslovi nastanka naponske korozije
(DUZS - Društvo za unapređivanje zavarivanja u Srbiji, Beograd, Srbija, 2012)
Opisani su osnovni mehanizmi naponske korozije različitih metala i legura i njihovih zavarenih spojeva. Detaljnije su
razmotreni metalurški i korozioni uslovi nastanka naponske korozije ugljeničnih i niskolegiranih čelika, ...
Synthesis of 4,6-dimethyl-3-cyano-2-pyridone catalysed by amino acids / Sinteza 4,6-dimetil-3-cijano-2-piridona katalizovana aminokiselinama
(Engineering Society for Corrosion, Belgrade, Serbia, 2017)
In this work the synthesis of 4,6-dimethyl-3-cyano-2-pyridone catalyzed by amino acids was studied. In the first part of the work, the optimization was carried out by varying the initial concentration of glycine, the molar ...
Analysis of the effects of butt welded joints on a carrying capacity of a structure tank / Analiza uticaja sučeono zavarenih spojeva na nosivost konstrukcije rezervoara
(Engineering Society for Corrosion, Belgrade, Serbia, 2017)
In the present paper, after calculation using the Finite Element Method (FEM), stress distribution on the model of a part of the pressure-tank mantle without welded joints (WJ), with transversal WJ, longitudinal WJ and ...
Behaviour of nionikral-70 in low-cycle fatigue
(Society for Structural Integrity and Life, Institute for Material Testing, 2017)
Experimental research on the behaviour of high-strength low-alloy steel ( HSLA)exposed to low-cycle fatigue (LCF) with controlled and fully reversible strain (Delta epsilon/2 = const, R epsilon =epsilon(min)/epsilon(max) ...
Integrated procedure for recycling and valorization of useful components from secondary raw materials based on hard metals
(Savez inženjera metalurgije Srbije, Beograd, 2017)
Wide application of hard metals requires increased consumption of their constituents. Their high cost and scarcity impose the need for finding new, both ecologically and economically justified ways for their production. ...
Failures of brass condenser tubes
(Society for Structural Integrity and Life, Institute for Material Testing, 2016)
Causes of failure of brass condenser tubes (CuZn28Sn1) in a thermal power plant in Serbia are analysed. Results of testing by Fourier transformed infrared spectroscopy (FTIR) have indicated the presence of ammonia and ...
Examination of the effectiveness of filtering half masks protection at various flow rates of aerosol contaminants / Ispitivanje efikasnosti zaštite filtrirajućih polumaski pri različitim protocima aerosolnih kontaminanata
(Engineering Society for Corrosion, Belgrade, Serbia, 2017)
The possibility of air contamination by biological agents, by natural or artificial way, requires the improvement and use of different means for respiratory protection. The paper presents comparative filtration efficiency ...
Corrosion properties of an aluminium alloy 7000 series after a new two step precipitation hardening / Otpornost prema koroziji aluminijumske legure serije 7000 posle novog dvostepenog termičkog taloženja
(Engineering Society for Corrosion, Belgrade, Serbia, 2014)
Corrosion properties of an aluminium alloy 7000 series were investigated by different electrochemical methods. The alloy was subjected to the one-step and to a new two-step precipitation hardening. Polarization measurements ...