Structure and Microstructure Characterization of the La2SrB10O19 Glass-ceramics
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2019)
The crystal structure of new lanthanum strontium borate glass-ceramics was refined by the Rietveld method. The results showed that La2SrB10O19 has the monoclinic crystal structure, space group C2 (No. 5) with a = 11.1170(6), ...
Mg/Cu co-substituted hydroxyapatite - Biocompatibility, mechanical properties and antimicrobial activity
(Elsevier Sci Ltd, Oxford, 2019)
The aim of this study was to improve the mechanical properties and to optimize antimicrobial activity of hydroxyapatite (HAP) by simultaneous doping with Mg and Cu ions in order to obtain material that would be able to ...
Change in structural, ferroelectric, and magnetic properties of bismuth ferrite induced by doping with gadolinium
(Elsevier Sci Ltd, Oxford, 2019)
Bismuth ferrite, BiFeO3, was doped with a wide range of concentrations (0-30%) of Gd in order to investigate structural, ferroelectric, and magnetic properties and their correlation. Powder samples of Bi1-xGdxFeO3 (x = ...
The effect of mechanical activation on synthesis and properties of MgAl2O4 ceramics
(Elsevier Sci Ltd, Oxford, 2019)
Magnesium aluminate, MgAl2O4 and other alumina-based spinels are ceramics with high hardness, high melting point and mechanical strenght. Spinels can also be used as dielectrics in microwave applications. The goal of this ...
Mg/Cu co-substituted hydroxyapatite – Biocompatibility, mechanical properties and antimicrobial activity
(Elsevier Ltd, 2019)
The aim of this study was to improve the mechanical properties and to optimize antimicrobial activity of hydroxyapatite (HAP) by simultaneous doping with Mg and Cu ions in order to obtain material that would be able to ...
Characterization of MgAl2O4 Sintered Ceramics
(Međunarodni Institut za nauku o sinterovanju, Beograd, 2019)
Single phase MgAl2O4 was made from a one-to-one molar ratio of MgO and Al2O3 powders mixed using ball-milling. Mixtures of MgO and Al2O3 were subsequently treated in planetary ball mill for 30, 60, 90 and 120 minutes in ...