Претраживање
Приказ резултата 1-10 од 13
Investigation of thermodynamic properties and phase equilibria in Ag-In-Sn system / Ispitivanje termodinamičkih veličina i faznih ravnoteža u sistemu Ag-In-Sn
(Savez inženjera i tehničara Srbije, Beograd, 2006)
Lead - free soldering became very popular in the whole world, because of high ecological demands in industry. Most of alternative alloys have high content of tin, and some of them are already used in electronic industry. ...
Examination of the adhesion of polymer composite films based on Bis-GMA/TEGDMA on different metal substrates / Ispitivanje adhezije polimernih kompozitnih filmova na bazi Bis-GMA/TEGDMA na različitim metalnim podlogama
(Savez inženjera i tehničara Srbije, Beograd, 2018)
The subject of this study is the quantitative adhesion of a UV-curing composite film based on Bis-GMA (Bisphenol A glycidylmethacrylate) / TEGDMA (triethylene glycol dimethacrylate) as a matrix and particles doped with ...
Examination of mechanical properties of acrilyc composite materials with different AL2O3 reinforcement by brazil test / Ispitivanje mehaničkih svojstava akrilatnih kompozitnih materijala sa različitim AL2O3 ojačanjima brazilskim testom
(Savez inženjera i tehničara Srbije, Beograd, 2019)
Composite materials based on UV-curing acrylates and various alumina-based reinforcements represent material that is suitable for the use in dentistry, but also in other areas. Composites were made using four different ...
Picosecond laser shock peening of base Nimonic 263 material and laser welded Nimonic 263 alloy / Mehanička obrada pikosekundnim laserom osnovnog materijala i zavarenih spojeva legure Nimonik 263
(DUZS - Društvo za unapređivanje zavarivanja u Srbiji, Beograd, 2015)
Laser welding is a welding process with a high energy density and numerous advantages over conventional welding methods (narrow heat affected zone, lower heat input, less distortion, and the like.) Mechanical treatment ...
Characterization of vacuum plasma spray VPS - W coating deposited on stainless steel substrates / Karakterizacija vakuum plazma sprej VPS - W prevlake deponovane na čeličnim podloga
(Inženjersko društvo za koroziju, 2021)
In this paper, studied was the melting of W powder particles in plasma, their behavior at oxidation as well as the mechanism of hardening on the surface of the substrate. Tungsten coating layers were deposited with vacuum ...
Characterisation of biocompatible layers of ZrO28%Y2O used in combination with other ceramics to modify the surface of implants / Karakterizacija biokompatibilnih slojeva ZrO28%Y2O3 koji se koriste u kombinaciji sa drugom keramikom za modifikaciju površine implantata
(Inženjersko društvo za koroziju, 2021)
The aim of this study was to deposit multi-functional ZrO28%Y2O3 coating layers using the plasma spray technology and then to characterise such layers. In combination with other biomedical ceramics, this coating is intended ...
Characterization of NiAl layers deposited by atmospheric plasma spray (APS) / Karakterizacija NiAl slojeva deponovanih atmosferskim plazma sprejom (APS)
(Engineering Society for Corrosion, Belgrade, Serbia, 2020)
In this paper analyzed were the mechanical properties and microstructure of the Ni30Al coating layers deposited using atmospheric plasma spray (APS). For deposition of the coating applied was a composite Ni30wt.% Al powder, ...
The mechanical and microstructural properties of VPS-Ti porous coating deposited on titanium alloy substrates for osseointegration / Mehanička i mikrostrukturna svojstva VPS-Ti porozne prevlake deponovane na podlogama od legure titana za osteointegraciju
(Engineering Society for Corrosion, Belgrade, Serbia, 2020)
The topography of the surface of the deposited VPS-Ti coatings on substrate surfaces of implants relating to the roughness and porous structure plays a decisive role in the process of on growth of the implants to the bones ...
Optimizing the content of nickel in flux-cored wire intended for welding micro-alloyed steels / Optimizacija sadržaja nikla u punjenoj žici namenjenoj za zavarivanje mikrolegiranih čelika
(DUZS - Društvo za unapređivanje zavarivanja u Srbiji, Beograd, 2014)
This paper presents the results related to organizing production of flux-cored wire alloyed with Ni and Mo according to standard AWS A5.29 intended for the MAG welding process. On the experimental line for steel strip ...
INTEGRITY AND RISK ASSESSMENT OF RECONSTRUCTED STEAM LINE / PROCENA INTEGRITETA I RIZIKA REKONSTRUISANOG PAROVODA
(Society for Structural Integrity and Life (DIVK), 2023)
The integrity assessment of high pressure steam pipeline
primarily requires stress state determination, including not
only effects of working pressure and temperature, but also
all acting loads. Toward this aim, the ...