Приказ резултата 1-10 од 13
Investigation of thermodynamic properties and phase equilibria in Ag-In-Sn system / Ispitivanje termodinamičkih veličina i faznih ravnoteža u sistemu Ag-In-Sn
(Savez inženjera i tehničara Srbije, Beograd, 2006)
Lead - free soldering became very popular in the whole world, because of high ecological demands in industry. Most of alternative alloys have high content of tin, and some of them are already used in electronic industry. ...
Examination of the adhesion of polymer composite films based on Bis-GMA/TEGDMA on different metal substrates / Ispitivanje adhezije polimernih kompozitnih filmova na bazi Bis-GMA/TEGDMA na različitim metalnim podlogama
(Savez inženjera i tehničara Srbije, Beograd, 2018)
The subject of this study is the quantitative adhesion of a UV-curing composite film based on Bis-GMA (Bisphenol A glycidylmethacrylate) / TEGDMA (triethylene glycol dimethacrylate) as a matrix and particles doped with ...
Examination of mechanical properties of acrilyc composite materials with different AL2O3 reinforcement by brazil test / Ispitivanje mehaničkih svojstava akrilatnih kompozitnih materijala sa različitim AL2O3 ojačanjima brazilskim testom
(Savez inženjera i tehničara Srbije, Beograd, 2019)
Composite materials based on UV-curing acrylates and various alumina-based reinforcements represent material that is suitable for the use in dentistry, but also in other areas. Composites were made using four different ...
Picosecond laser shock peening of base Nimonic 263 material and laser welded Nimonic 263 alloy / Mehanička obrada pikosekundnim laserom osnovnog materijala i zavarenih spojeva legure Nimonik 263
(DUZS - Društvo za unapređivanje zavarivanja u Srbiji, Beograd, 2015)
Laser welding is a welding process with a high energy density and numerous advantages over conventional welding methods (narrow heat affected zone, lower heat input, less distortion, and the like.) Mechanical treatment ...
Characterization of vacuum plasma spray VPS - W coating deposited on stainless steel substrates / Karakterizacija vakuum plazma sprej VPS - W prevlake deponovane na čeličnim podloga
(Inženjersko društvo za koroziju, 2021)
In this paper, studied was the melting of W powder particles in plasma, their behavior at oxidation as well as the mechanism of hardening on the surface of the substrate. Tungsten coating layers were deposited with vacuum ...
Optimizing the content of nickel in flux-cored wire intended for welding micro-alloyed steels / Optimizacija sadržaja nikla u punjenoj žici namenjenoj za zavarivanje mikrolegiranih čelika
(DUZS - Društvo za unapređivanje zavarivanja u Srbiji, Beograd, 2014)
This paper presents the results related to organizing production of flux-cored wire alloyed with Ni and Mo according to standard AWS A5.29 intended for the MAG welding process. On the experimental line for steel strip ...
The mechanical and microstructural properties of VPS-Ti porous coating deposited on titanium alloy substrates for osseointegration / Mehanička i mikrostrukturna svojstva VPS-Ti porozne prevlake deponovane na podlogama od legure titana za osteointegraciju
(Engineering Society for Corrosion, Belgrade, Serbia, 2020)
The topography of the surface of the deposited VPS-Ti coatings on substrate surfaces of implants relating to the roughness and porous structure plays a decisive role in the process of on growth of the implants to the bones ...
Characterization of plasma spray bioinert coating Al2O328wt.%MgO / Karakterizacija plazma sprej bioinertne prevlake Al2O328tež.%MgO
(Engineering Society for Corrosion, Belgrade, Serbia, 2019)
This paper presents the results of testing mechanical and structural characteristics of plasma spray coating Al2O328wt.%MgO. Metal oxide MgO in a complex oxide Al2O328wt.%MgO modifies the properties of Al2O3 ceramics by ...
Mechanical properties and microstructure of the ZrO25CaO/NiCrAl coating system / Mehaničke osobine i mikrostruktura sistema prevlaka ZrO25CaO/NiCrAl
(Engineering Society for Corrosion, Belgrade, Serbia, 2019)
ZrO25CaO is a versatile class of material that can be sintered or plasma spray deposited in combination with other materials on the implant substrate. Due to brittleness the organic ceramic hydroxyapatite Ca10(PO4)6(OH)2 ...
Mechanical properties and microstructure of molybdenum coating layers deposited vacuum plasma spray process / Mehanička svojstva i mikrostruktura slojeva prevlake molibdena deponovane vakuum plazma sprej procesom
(Engineering Society for Corrosion, Belgrade, Serbia, 2019)
Molybdenum coatings due to their excellent wear resistant properties and sliding characteristics under dry friction conditions are often used in applications to resist friction and dry sliding. Since molybdenum metal is ...